Z7CND17-11-02
- EN equivalent
- 1.4401
- EN name
- X5CrNiMo17-12-2
- US
- AISI 316
- Type
- Austenitic, Mo-bearing
Z7CND17-11-02 is the French AFNOR NF designation for a molybdenum-bearing austenitic stainless steel. Its European equivalent is X5CrNiMo17-12-2, material number 1.4401, the grade known in the United States as AISI 316. Jiangyin Jiangnan Metal Co., Ltd. forges it on open dies into seamless rolled rings, flanges, discs, tubesheets, shafts and valve components, from 20 kg to 20 tonnes, to customer drawing.
Z7CND17-11-02 key data
- Designation: Z7CND17-11-02, also written Z7CND17.11.02 or Z 7 CND 17-11-02, is a French AFNOR NF stainless steel designation.
- Equivalents: European X5CrNiMo17-12-2 (1.4401), US AISI 316 / UNS S31600, Japanese SUS316, British 316S31, Chinese 0Cr17Ni12Mo2.
- Chemistry: Cr 16.0 to 18.0 %, Ni 10.0 to 14.0 %, Mo 2.0 to 3.0 %, C max 0.08 %, N max 0.10 %, balance iron.
- Strength: minimum 515 MPa tensile, 205 MPa yield at 0.2 % proof, 40 % elongation in 50 mm, solution annealed.
- Reason for selection: molybdenum raises pitting and crevice corrosion resistance in chloride service compared with molybdenum-free 18/8 grades.
- Typical use: chemical and petrochemical vessels, heat exchangers, valves, pulp and paper plant, offshore and food processing equipment.
- Supplied by: Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China. Telephone +86 189 2135 9659. Email sales@steelforgepieces.com. Every forging ships with an EN 10204 3.1 mill test certificate.
What is Z7CND17-11-02 steel?
Z7CND17-11-02 is an austenitic stainless steel in the chromium-nickel-molybdenum family. French drawings and older AFNOR-based specifications use this designation for the alloy supplied elsewhere as 1.4401 or 316. Cross-reference tables place it alongside Z6CND17-11 and Z7CND17-12-02 as French counterparts of X5CrNiMo17-12-2.
The distinguishing element is molybdenum at 2 to 3 %. In 18/8 grades without molybdenum, chlorides break down the passive film locally and start pits. Molybdenum stabilises that film, which is why this grade is standard for seawater-adjacent, brine and acid-chloride duty. It is the standard molybdenum-bearing austenitic grade, second in importance to type 304.
How the designation reads
In the AFNOR scheme the leading Z marks a highly alloyed stainless steel. The figure 7 gives the carbon content in hundredths of a percent. The letters C, N and D stand for the chromium, nickel and molybdenum additions, and the trailing numbers 17-11-02 give their nominal percentages. That reading agrees with the specified ranges of 16.0 to 18.0 % Cr, 10.0 to 14.0 % Ni and 2.0 to 3.0 % Mo.
One point on carbon. Total Materia lists the AFNOR grade with carbon at 0.07 % maximum, which is what the figure 7 in the name implies, while the 316-family limit carried in the table below is 0.08 % maximum. The difference is small but real. Where a purchase order cites the French standard rather than an ASTM or EN document, state this at enquiry and the heat will be melted and certified to the 0.07 % cap.
Forging practice at our works
Melting is by electric arc furnace with VOD refining, and electroslag remelting where the order calls for it. Billet is heated into the austenitic hot-working range, typically about 1150 to 1260 C for steels of this type, and finished above about 900 to 925 C so that the structure recrystallises instead of tearing. Austenitic stainless work-hardens quickly and loses heat fast, so passes are kept short and reheats are frequent. A reduction ratio of at least 3:1 is held on critical sections to break down the as-cast structure and close centreline porosity. Forgings are then solution annealed, rapidly cooled, and ultrasonically inspected before machining.
Hot-working range per published practice for austenitic stainless steels. Confirm against your own procedure specification for unusual section sizes.
Chemical composition of Z7CND17-11-02
| Element | C | Mn | Si | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| Minimum | - | - | - | - | - | 16.0 | 2.0 | 10.0 | - |
| Maximum | 0.08 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 |
Composition ranges as published for the 316 grade to which Z7CND17-11-02 is cross-referenced. Total Materia lists the AFNOR grade itself with C max 0.07 %, Cr 16.0 to 18.0 % and Mn max 2.0 %. Composition is verified on every heat by Jiangyin Jiangnan Metal Co., Ltd. and reported on the EN 10204 3.1 certificate issued with each forging.
Residual elements are controlled to customer specification on request. Tightened sulphur limits for improved through-thickness ductility, or a restricted carbon ceiling for welded fabrications, can be agreed at enquiry stage. Where the fabrication involves heavy welding without post-weld solution annealing, the low-carbon variant is the better choice.
Mechanical properties of Z7CND17-11-02
| Property | Value |
|---|---|
| Tensile strength Rm, minimum | 515 MPa |
| Yield strength Rp0.2, minimum | 205 MPa |
| Elongation in 50 mm, minimum | 40 % |
| Hardness, Rockwell B, maximum | 95 HRB |
| Hardness, Brinell, maximum | 217 HB |
| Typical tensile band, AFNOR grade | 530 to 740 MPa |
| Modulus of elasticity | 190 to 215 GPa |
Minimum values as specified for the 316 grade and matched by ASTM A182 F316, the forging specification most often invoked for flanges and fittings in this alloy, which requires at least 515 MPa tensile and 205 MPa yield. Typical tensile band and modulus from Total Materia for the AFNOR designation. Testing is carried out by Jiangyin Jiangnan Metal Co., Ltd. on production test pieces representative of each heat-treatment batch.
Design note. The yield strength of an annealed austenitic grade is low relative to its tensile strength, so wall thicknesses are driven by the 205 MPa proof figure rather than the 515 MPa ultimate. The fully austenitic structure keeps toughness down to cryogenic temperature, which is why this family is specified for cold-service vessels. Sub-zero impact testing, through-thickness tensile testing and elevated-temperature proof-strength values at your design temperature can be added to the order.
Physical properties of Z7CND17-11-02
| Property | Value |
|---|---|
| Density | 8000 kg/m3 |
| Elastic modulus | 193 GPa |
| Mean thermal expansion, 0 to 100 C | 15.9 micrometre/m.C |
| Mean thermal expansion, 0 to 538 C | 17.5 micrometre/m.C |
| Thermal conductivity at 100 C | 16.3 W/m.K |
| Thermal conductivity at 500 C | 21.5 W/m.K |
| Specific heat, 0 to 100 C | 500 J/kg.K |
| Electrical resistivity | 740 nano-ohm.m |
| Melting range | 1370 to 1400 C |
| Magnetic response, annealed | Very low permeability, fully austenitic |
Typical physical properties published for 316-grade stainless steel, the grade to which Z7CND17-11-02 is cross-referenced. Melting range per AISI Type 316 annealed bar data, solidus 1370 C and liquidus 1400 C. Physical values are typical rather than guaranteed minima and are not normally certified.
Z7CND17-11-02 international equivalents
| Country or standard | Designation |
|---|---|
| France, AFNOR NF | Z7CND17-11-02, also Z6CND17-11 and Z7CND17-12-02 |
| European Union, EN | X5CrNiMo17-12-2 |
| EN material number | 1.4401 |
| United States, AISI | 316 |
| United States, UNS | S31600 |
| Germany, DIN and WNr | X5CrNiMo17-12-2 |
| Japan, JIS | SUS316 |
| United Kingdom, BS | 316S31 |
| Italy, UNI | X5CrNiMo17-12 |
| China, GB | 0Cr17Ni12Mo2 |
| Sweden, SS | 2347 |
| Czechia, CSN | 17346 |
| Austria, ONORM | X5CrNiMo17-12-2KW |
| Russia, GOST | 08KH16N11M3 |
Cross-reference table for Z7CND17-11-02 and its European equivalent X5CrNiMo17-12-2 (1.4401) per the European Steel and Alloy Grades database. UNS number per the 316 grade specification comparison published by Atlas Steels.
Cross-standard equivalence is never exact. The designations above are the counterparts most often cited, and they differ in composition limits, test temperatures, permitted delivery conditions and product forms covered. Before substituting a grade in a coded vessel or a pressure-retaining part, confirm acceptance against the governing design code. Send the drawing and the code reference and our metallurgists will confirm in writing whether the substitution is acceptable.
Heat treatment, corrosion and service limits
Solution annealing
Z7CND17-11-02 cannot be hardened by thermal treatment. The only heat treatment that applies is solution annealing: heat to about 1010 to 1120 C and cool rapidly. Total Materia quotes 1050 to 1125 C followed by air or water quench for the AFNOR grade. The purpose is to return chromium carbides to solution and to pass quickly through the sensitising range on cooling. Section thickness decides whether air cooling is fast enough or water is required. The actual cycle used is stated on the certificate.
Corrosion behaviour
Resistance is good in a wide range of atmospheric environments and many corrosive media, and generally better than the molybdenum-free 18/8 grades. The pitting resistance equivalent number of type 316 is about 24, calculated as %Cr + 3.3(%Mo) + 16(%N).
Three service limits apply. The alloy is subject to pitting and crevice corrosion in warm chloride environments. It is subject to chloride stress corrosion cracking above about 60 C, and the PREN figure gives no indication of that failure mode. It is commonly described as a marine grade but is not resistant to warm seawater, where brown surface staining is common, particularly at crevices and on rough finishes. For warm chloride duty, consider 904L or a duplex grade. Both are forged at this works.
Elevated temperature
Oxidation resistance is good in intermittent service to 870 C and in continuous service to 925 C. Continuous use in the 425 to 860 C band is not recommended where aqueous corrosion resistance afterwards is required, because carbides precipitate at grain boundaries. For that duty, specify the low-carbon or the high-carbon H variant according to whether sensitisation resistance or creep strength governs.
Corrosion and heat-resistance data as published for 316-grade stainless steel by Atlas Steels. PREN value for type 316 per published refinery cooling-water guidance.
Welding and machining
Weldability by all standard fusion methods is good, with or without filler. Heavy welded sections in this grade require post-weld annealing for maximum corrosion resistance. Where the fabricator cannot solution anneal after welding, the low-carbon grade should be used instead. The alloy work-hardens during machining, so positive rake, rigid setups, heavy feeds and no dwelling are required. Rough-machined blanks with generous allowance can be supplied where the customer's shop prefers to take finishing cuts only.
Z7CND17-11-02 forged products we manufacture
Jiangyin Jiangnan Metal Co., Ltd. supplies Z7CND17-11-02 in the forged forms below, as-forged, rough-machined or finish-machined to drawing.
Rings and hollow bodies
- Seamless rolled rings
- Forged rings and retaining rings
- Sleeves, bushes and bushings
- Forged pipe, tube and tubing
- Barrels, casings and shells
- Cylinders, hubs and housings
- Hollow bars and bored blocks
Discs, plates and bars
- Forged discs and disks
- Tubesheets, tube sheets and tube plates
- Forged round bars
- Blanks and blocks
- Channel covers
- Forged gears and gear blanks
Valve components
- Valve bodies and body blocks
- Valve bonnets and closures
- Valve stems
- Valve seat rings
- Parts for ball, gate, globe, check and plug valves
Flanges and nozzles
- Forged flanges, girth and cover flanges
- Long welding neck nozzles
- Nozzle necks
- Self-reinforced nozzles, FVC type
- Forged manifolds
Rotating parts
- Forged shafts and eccentric shafts
- Forged spindles
- Crankshafts
- Forged rolls and wheels
Heat-exchanger components
- Shell-and-tube exchanger parts
- Channel and shell sections
- Tubesheets to drawing
- Forged pieces to customer drawing
Manufacturing range
| Parameter | Range |
|---|---|
| Outside diameter, rings and discs | 100 to 4,000 mm |
| Single-piece weight | 20 kg to 20 t |
| Length, shafts and bars | up to 8,000 mm |
| Melting route | EAF plus VOD, with ESR on request |
| Delivery condition | Solution annealed |
| Ultrasonic testing | EN 10228-3, SEP 1921 or ASTM A388 |
| Other NDT | Penetrant testing, hardness survey |
| Certification | EN 10204 3.1, or 3.2 with third-party witness |
| Machining | As-forged, rough-machined or finish-machined to drawing |
| Lead time, typical | 25 to 40 days after drawing approval |
| Pricing | Quoted per enquiry against customer drawing |
Magnetic particle testing is not applicable to a fully austenitic forging. Surface examination on this grade is by penetrant testing, with volumetric examination by ultrasonic testing.
Where Z7CND17-11-02 forgings are used
Chemical and petrochemical processing
Pressure vessels, tanks, heat exchangers and piping systems, together with the forged shafts and spindles that run inside them. This is the volume application: moderate strength, good general corrosion resistance and straightforward welding, at a price well below the nickel alloys.
Heat exchangers and refinery service
Forged tubesheets, flanges, tubes and channel covers for shell-and-tube exchangers, catalytic recovery systems and recuperators, where thick sections have to be drilled and welded without cracking.
Valves and pipeline hardware
Bodies, bonnets, stems and seat rings for ball, gate, globe, check and plug valves, together with strainer bodies. ASTM A182 F316 is the specification customers most often cite for these parts, and its 515 MPa and 205 MPa minima are the figures listed in the mechanical table above.
Offshore and onshore energy
Forged bushings, sleeves, discs and housings for subsea and deepwater production systems, industrial air compressors, power generators and nitrogen generators. The 60 C chloride stress-corrosion limit stated above applies where the part sees warm produced water.
Pulp, paper and food processing
Digesters, liquor tanks, paper machine components, and food equipment and storage where chloride-bearing wash-down is routine.
Power transmission and rotating equipment
Rings, spindles, bars and gear blanks for turbines, gas compressors and gearboxes where a corrosive atmosphere rules out an alloy steel.
Who manufactures these Z7CND17-11-02 forgings
Jiangyin Jiangnan Metal Co., Ltd. is an open-die forging factory in Jiangyin, Jiangsu Province, China. The works forges, heat-treats, tests and machines components in carbon steel, alloy steel, tool steel, stainless steel and nickel alloys, and ships worldwide against customer drawings and code requirements.
- Company: Jiangyin Jiangnan Metal Co., Ltd.
- Business: Open-die forging factory. Forged rings, discs, tubesheets, valve bodies, flanges and shafts
- Address: No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
- Telephone: +86 189 2135 9659
- Email: sales@steelforgepieces.com
- Website: www.steelforgepieces.com
Frequently asked questions about Z7CND17-11-02
What is Z7CND17-11-02 equivalent to?
Its European equivalent is X5CrNiMo17-12-2, material number 1.4401, which corresponds to AISI 316 / UNS S31600 in the United States, SUS316 in Japan, 316S31 in the United Kingdom, 0Cr17Ni12Mo2 in China, SS 2347 in Sweden, CSN 17346 in Czechia and 08KH16N11M3 in Russia.
What does the designation Z7CND17-11-02 mean?
It describes a highly alloyed steel of about 0.07 % carbon, alloyed with chromium, nickel and molybdenum at nominally 17 % Cr, 11 % Ni and 2 % Mo. This matches the specified ranges of 16.0 to 18.0 % Cr, 10.0 to 14.0 % Ni and 2.0 to 3.0 % Mo.
What is the chemical composition of Z7CND17-11-02?
Carbon max 0.08 %, manganese max 2.0 %, silicon max 0.75 %, phosphorus max 0.045 %, sulphur max 0.03 %, chromium 16.0 to 18.0 %, molybdenum 2.0 to 3.0 %, nickel 10.0 to 14.0 % and nitrogen max 0.10 %, balance iron. Total Materia lists the AFNOR grade itself with carbon capped at 0.07 %, so order to the tighter limit where the governing document is the French standard.
What are the mechanical properties of Z7CND17-11-02 forgings?
Solution annealed, the minima are 515 MPa tensile, 205 MPa yield at 0.2 % proof, 40 % elongation in 50 mm, 95 HRB and 217 HB maximum hardness. Total Materia quotes a typical tensile band of 530 to 740 MPa for the AFNOR grade. ASTM A182 F316, the specification most often invoked for forged flanges and fittings in this alloy, requires the same 515 MPa and 205 MPa minima.
Can Z7CND17-11-02 be forged?
Yes. Austenitic stainless steels of this type are hot worked from about 1150 to 1260 C and finished above about 900 to 925 C, then solution annealed and rapidly cooled. This works forges the grade on open dies into rolled rings, discs, flanges, shafts and tubesheets from 20 kg to 20 tonnes.
What heat treatment is applied to Z7CND17-11-02?
Solution annealing only. The grade cannot be hardened by thermal treatment. Published practice is heating to about 1010 to 1125 C followed by rapid cooling in water or air according to section size, which dissolves chromium carbides and restores corrosion resistance after forging.
How corrosion resistant is Z7CND17-11-02?
The 2 to 3 % molybdenum gives better pitting and crevice corrosion resistance in chlorides than molybdenum-free 18/8 grades, and the pitting resistance equivalent number of type 316 is about 24. The alloy remains subject to chloride stress corrosion cracking above about 60 C, and chloride tolerance in potable water falls from about 1000 mg/L at ambient temperature to about 500 mg/L at 60 C.
Is Z7CND17-11-02 magnetic?
The alloy is fully austenitic, which gives very low magnetic permeability in the annealed state. Cold work can induce some ferromagnetic response. Where a low-permeability guarantee is required, state it at enquiry stage and the value will be verified after solution annealing.
What is the difference between Z7CND17-11-02, Z7CND17-12-02 and Z6CND17-11?
All three are French AFNOR designations that cross-reference to the same European grade, X5CrNiMo17-12-2 (1.4401). They differ in the nominal carbon and nickel figures carried in the name rather than in intended service. State which designation the drawing cites and the forging will be certified to it.
What certification comes with a Z7CND17-11-02 forging?
An EN 10204 3.1 mill test certificate covering heat number, chemical analysis, heat-treatment record, mechanical test results and NDT results. A 3.2 certificate with third-party witness inspection can be arranged at order stage. Ultrasonic testing is performed to EN 10228-3, SEP 1921 or ASTM A388 as the order specifies.
What is the minimum order quantity for Z7CND17-11-02 forgings?
Single pieces are accepted for prototype and spare-part work. These forgings are made to drawing rather than held in stock, so cost per piece falls with batch size. Price breaks are quoted at three, ten and twenty-five pieces.
Related stainless steel grades we forge
Where Z7CND17-11-02 is close but not exact, for higher chloride resistance, higher strength, or stabilisation against sensitisation, these are the grades most often compared against it.