Super Austenitic Stainless Steel
UNS S32654 Forgings 654 SMO · W.Nr 1.4652 · X1CrNiMoCuN24-22-8
Rolled rings, flanges, bars, discs, sleeves, shafts and tube sheets in the highest-alloyed super austenitic grade in common use. We melt the steel, forge it, solution anneal it and machine it on one site in Jiangyin, so the certificate traces back to a heat number rather than to a purchased billet.
UNS S32654, sold as 654 SMO and designated EN 1.4652, is a conventionally melted super austenitic stainless steel with roughly 24 to 25 percent chromium, 21 to 23 percent nickel, 7 to 8 percent molybdenum and 0.45 to 0.55 percent nitrogen. It is the most highly alloyed member of the SMO super austenitic family, and its resistance to pitting, crevice corrosion and chloride stress corrosion cracking comes close to that of nickel-based alloys. Buyers reach for it when a 6 percent molybdenum grade such as S31254 or 904L has already failed, or is predicted to fail, in hot seawater, concentrated brine or chlorinated acid service. Jiangyin Jiangnan Metal Co., Ltd. forges the grade to drawing at its works in Jiangyin, Jiangsu, China.
Grade identity
One alloy, several names. Enquiries arrive under all of them and they refer to the same chemistry.
| System | Designation | Note |
|---|---|---|
| UNS | S32654 | Primary designation used in ASTM and ASME work |
| EN / Werkstoff | 1.4652 | European number, used in EN 10216-5 and EN 10217-7 |
| EN name | X1CrNiMoCuN24-22-8 | Reads the chemistry directly |
| Trade name | 654 SMO | Originating producer designation, Outokumpu |
| Shorthand | 7Mo, Alloy 654 | Common in trading and older enquiry documents |
| JIS, GOST, GB | No direct listing | Grade sits above the range of those standards; supplied against UNS or EN chemistry |
654 SMO is a trademark of its owner and appears here only to identify the grade. Material is supplied to the UNS S32654 and EN 1.4652 chemistry, not under any third-party brand.
Chemical composition
The manganese figure is the one people query. It is high on purpose. Nitrogen at 0.45 to 0.55 percent will not stay in solution without it, and the nitrogen is where most of the strength and a large share of the pitting resistance comes from.
| Element | Range | Why it is there |
|---|---|---|
| Carbon | 0.020 max | Held low against carbide precipitation at grain boundaries |
| Chromium | 24.0 – 25.0 | Passive film, first term in the PREN calculation |
| Nickel | 21.0 – 23.0 | Keeps the structure austenitic at this alloy level, resists chloride cracking |
| Molybdenum | 7.0 – 8.0 | Largest single contributor to pitting and crevice resistance |
| Nitrogen | 0.45 – 0.55 | Strength and pitting resistance, roughly twice the level in S31254 |
| Manganese | 2.0 – 4.0 | Raises nitrogen solubility so the nitrogen stays in the melt |
| Copper | 0.30 – 0.60 | Helps in reducing conditions, sulphuric acid in particular |
| Silicon | 0.50 max | Deoxidation |
| Phosphorus | 0.030 max | Residual limit |
| Sulphur | 0.005 max | Tight, for hot workability and clean inclusion rating |
Copper is quoted as 0.30 to 0.60 in most forging and plate specifications. At least one published datasheet lists copper as 0.30 maximum. Confirm which window your specification applies before order and the heat will be aimed at it.
Mechanical and physical properties
Figures below are minima in the solution annealed condition. The yield strength is the commercially interesting number: close to double that of 316L, which is what lets a designer take wall thickness out of a high pressure brine component while gaining corrosion margin at the same time.
| Property | Metric | Imperial |
|---|---|---|
| Tensile strength, min | 750 MPa | 109 ksi |
| Yield strength, 0.2 % offset, min | 430 MPa | 62 ksi |
| Elongation, min | 40 % | 40 % |
| Hardness, annealed | approx. 220 HB max | — |
| Density | 8.0 g/cm³ | 0.289 lb/in³ |
| Structure | Fully austenitic, non-magnetic as annealed, not hardenable by heat treatment | |
ASTM A312 lists the same 750 MPa and 430 MPa minima with 35 percent elongation rather than 40. Where a specification is named on the purchase order, that specification governs and the test certificate is issued against it.
Corrosion behaviour and PREN
PREN is calculated as %Cr + 3.3 × %Mo + 16 × %N. Figures published for S32654 do not agree, because they are calculated from different points in the composition range. Langley Alloys publishes 54. Datasheets working from the top of the range publish 63 to 64. Rather than quote the largest number, the honest statement is that S32654 lands between the mid-fifties and the low sixties depending on the heat, and that in every published comparison it sits well clear of the 6 percent molybdenum grades.
| Grade | UNS | Molybdenum | PREN |
|---|---|---|---|
| 316L | S31603 | approx. 2 % | 25 |
| 254 SMO / Alloy 254 | S31254 | approx. 6 % | 43 |
| 654 SMO | S32654 | 7 – 8 % | 54 to above 60, source dependent |
What we forge in S32654
Every item is forged from one piece of steel. No welding, no casting, no billet of unknown origin.
Size envelope
The limits below are the plant maximums across all grades. S32654 is a hard alloy to work, so the usable envelope in this grade is narrower, and each enquiry is reviewed against the drawing before a size is confirmed.
| Item | Limit | Set by |
|---|---|---|
| Rolled ring outside diameter | up to 6,000 mm | 6 m radial-axial ring mill |
| Minimum ring size | from OD 50 mm | Upset and punch route below ring mill range |
| Single piece weight | up to 30,000 kg | 60 t heat, 6,300 t press |
| Machined diameter | up to 5,000 mm | 5,000 mm vertical turning lathe |
| Shaft turned length | up to 14,000 mm | C61160 horizontal lathe, 15 m well furnace for vertical quench |
| Bored cylinders | 1,600 mm dia × 10,000 mm | CNC deep-hole drilling machine |
| Minimum order | 10 kg | No minimum piece count |
Melting, forging, heat treatment
Melting
Most forging suppliers in China buy billet. This works starts at the furnace. S32654 runs through the electric arc furnace, is refined in the ladle furnace, then decarburised under vacuum, which is the step that matters here: vacuum oxygen decarburisation is how carbon is pulled to 0.020 percent maximum while nitrogen is held at 0.45 to 0.55 percent. Where the order calls for it, the heat is electroslag remelted under protective atmosphere for inclusion cleanliness. Maximum heat size is 60 tonnes.
Forging
S32654 keeps its strength at temperature and has a short hot working window, so passes are planned to avoid finishing cold. Sigma and other intermetallic phases form in the region of 700 to 900 degrees Celsius, and time spent there during forging and cooling is kept down. Presses available are 6,300 t, 4,000 t and 2,000 t, with ring mills at 6 m, 3 m and 1 m.
Heat treatment
Solution anneal near 1150 to 1200 degrees Celsius, then rapid water quench. This returns intermetallics to solution and restores the corrosion resistance the alloy is bought for. The grade takes no precipitation hardening treatment. Fourteen furnaces are on site, including car-bottom furnaces to 8,000 × 2,000 × 2,000 mm and 15 m deep well furnaces for vertical quenching of long parts.
Note for fabricators
Where our forgings are welded into an assembly, a nickel-based filler of the ERNiCrMo type is normally used so that the weld metal does not become the weakest point in the corrosion chain.
Where it gets used
This is an expensive alloy and it is only specified where the environment pays for it. The established markets are these.
| Sector | Application | Reason for the grade |
|---|---|---|
| Desalination | Brine heater internals, high pressure brine piping, MSF and MED plant, reverse osmosis high pressure sections | Brine concentration and temperature beyond what 254 SMO and 904L will take |
| Offshore oil and gas | Seawater and firewater systems, produced water handling, risers, manifolds, subsea connectors | Chloride plus temperature plus pressure; the strength reduces dependence on cathodic protection |
| Chlor-alkali and chemical | Chlorine and chlorine dioxide duty, sulphuric and mixed acid equipment carrying chlorides, heat exchanger parts | Oxidising and high chloride conditions at the same time |
| Pulp and paper | Black liquor evaporator bodies and internals in kraft mills | Alkaline chloride cracking resistance at temperature |
| Power | Flue gas desulphurisation absorbers and ducting components | Acidic chloride condensate |
| Water treatment | Demineralised water plant, waste water, high salinity process equipment | Design life in chloride bearing water |
Standards, testing, certification
| Form | ASTM / ASME | European |
|---|---|---|
| Plate, sheet, strip | A240 / SA240 | EN 10088 |
| Seamless pipe | A312 | EN 10216-5 |
| Heat exchanger tube | A213 | EN 10216-5 |
| General tubing | A269 | — |
| Welded tube | A249 | EN 10217-7 |
| Forgings and rolled rings | Supplied to the grade chemistry and property requirements with A182 style supplementary requirements applied by agreement. Tell us the exact forging specification your project names and we will confirm in writing whether we can certify to it before you place the order. | |
| Check | Standard or scope |
|---|---|
| Ultrasonic testing | EN 10228-3, SEP 1921, ASTM A388 |
| Chemical analysis | Optical emission spectrometry on every heat; handheld PMI on request |
| Mechanical testing | Tensile, yield, elongation, hardness; Charpy impact on request |
| Corrosion testing | ASTM G48 pitting and critical pitting temperature, placed with an accredited laboratory |
| Certification | EN 10204 3.1 as standard. 3.2 witnessed by BV, DNV, LR, SGS or TUV on request |
| Works approvals | CCS, BV, DNV, LR, NK |
| Dimensional | Full report against customer drawing |
Questions we are asked
Is S32654 a powder metallurgy steel?
No, and this is worth correcting because the claim is copied across a number of supplier pages. S32654 is a conventionally melted wrought stainless steel. We produce forging stock by electric arc melting with ladle refining and vacuum oxygen decarburisation, with electroslag remelting added where the specification asks for it.
How does it differ from 254 SMO?
S32654 carries 7 to 8 percent molybdenum against roughly 6 in S31254, more chromium, and about twice the nitrogen. That buys both a higher PREN and a considerably higher yield strength. The usual trigger for switching is a 6 percent molybdenum grade that has already pitted in service, or a duty where the design seawater temperature rules one out on paper.
Can it replace a nickel alloy or titanium?
In a lot of chloride service its localised corrosion resistance is in the same band as the better nickel alloys, and it is regularly evaluated as a cheaper substitute in seawater and brine systems. Whether the swap holds depends on the actual temperature, chloride level, pH, and whether reducing acids or hydrogen sulphide are present. It is a case-by-case decision, not a general rule.
Do you hold S32654 in stock?
Not as finished forgings. This grade is made to order against the drawing, which is the normal arrangement for a 7 percent molybdenum alloy. Lead time runs 20 to 60 days depending on size, heat treatment and testing scope.
What do you need to quote?
Finished size or forged size, or a drawing. Quantity. The specification the project names. Any testing beyond our standard scope, and whether 3.1 or 3.2 certification is required. Quotations normally go back within one working day.
Request a quotation