AISI 317LM Forgings: UNS S31725 / ASTM A182 Grade F47
Rolled rings, forged flanges, round bars, shafts, discs, sleeves and tube sheets, open-die forged to drawing by Jiangyin Jiangnan Metal Co., Ltd.
Grade in short. AISI 317LM is a low-carbon, high-molybdenum austenitic stainless steel, UNS S31725, listed in ASTM A182/A182M as forging grade F47. The forging chemistry is 18.0-20.0 % Cr, 13.0-17.5 % Ni, 4.0-5.0 % Mo, carbon 0.030 % max and nitrogen 0.10 % max. The molybdenum level puts the calculated PREN near 35, well above 304 and 316, and the grade was developed in particular to handle sulfuric acid compounds. It stays fully austenitic, is not hardenable by heat treatment, and forges readily.
Where to buy. Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China, forges 317LM / S31725 / A182 F47 to customer drawing with EN 10204 3.1 or 3.2 certification and ultrasonic testing to EN 10228-3, SEP 1921 or ASTM A388. Enquiries: sales@steelforgepieces.com, +86 189-2135-9659.
1. Designations and equivalents
| System | Designation | Remarks |
|---|---|---|
| AISI / trade name | 317LM | Also written 317 LM, 317LMG |
| UNS | S31725 | Primary identifier |
| ASTM A182/A182M | F47 | Forged flanges, fittings, valves and parts |
| Other ASTM product forms | A240 plate, A276 and A479 bar, A312, A213, A249, A269 tube and pipe, A358, A376, A409, A167 | Same chemistry, different product-form rules |
| EN reference | 1.4439 / X2CrNiMoN17-13-5 | Conversion tables disagree, see note below |
| Neighbouring grades | 317L (S31703, EN 1.4438), 317LMN (S31726) | 317LMN is the nitrogen-alloyed version |
2. Chemical composition
| Element | ASTM A182 F47 / S31725 | General 317LM datasheet |
|---|---|---|
| Carbon, C | 0.030 max | 0.03 max |
| Chromium, Cr | 18.0 - 20.0 | 18 - 20 |
| Nickel, Ni | 13.0 - 17.5 | 12 - 16 |
| Molybdenum, Mo | 4.0 - 5.0 | 4 - 5 |
| Manganese, Mn | 2.00 max | 2.00 max |
| Silicon, Si | 0.75 max | 1.00 max |
| Nitrogen, N | 0.10 max | not specified |
| Phosphorus, P | 0.045 max | 0.045 max |
| Sulfur, S | 0.030 max | 0.03 max |
| Iron, Fe | Balance | Balance |
The two columns differ in the nickel and silicon windows because the A182 forging table and the general grade datasheet were written for different product scopes. For forgings the A182 F47 column governs. Pitting resistance equivalent, calculated as %Cr + 3.3 x %Mo + 16 x %N, works out at roughly 35 for this chemistry.
3. Mechanical properties
| Property | ASTM A182 F47 forgings | Plate and general datasheet |
|---|---|---|
| Tensile strength, min | 525 MPa / 75 ksi | 515 MPa / 74 ksi |
| Yield strength 0.2 %, min | 205 MPa / 30 ksi | 205 MPa / 30 ksi |
| Elongation, min | 40 % in 2 in. or 4D | 35 % |
| Reduction of area, min | 50 % | not specified |
| Hardness, annealed | about 95 HRB | |
| Modulus of elasticity | 190 - 210 GPa | |
| Poisson's ratio | 0.27 - 0.30 | |
| Density | 7.7 - 8.03 g/cm3 | |
4. Forging, heat treatment, machining, welding
Hot working
Heat to 1149-1260 C (2100-2300 F). Do not continue working below about 927 C (1700 F). A post-work anneal is advised for optimum corrosion resistance.
Solution annealing
Soak at 1121-1149 C (2050-2100 F), then water quench. The grade takes no hardening heat treatment; strength rises only through cold reduction.
Machining
Low speeds and constant feed keep work hardening down. 317LM is tougher than 304 and throws a long stringy chip, so chip breakers are recommended.
Welding
All conventional processes apply. Published filler recommendations are 317L or alloy 625 type consumables where matching or over-alloyed weld metal is wanted.
Forming takes roughly twice the force of a standard austenitic grade, ample radii should be allowed in roll forming, and cuts have to go through the full thickness because the material does not snap.
5. Corrosion behaviour
317LM was designed against sulfuric acid attack, and the 4-5 % molybdenum also lifts resistance to chlorides, pitting and crevice corrosion compared with 304 and 316. Carbon held at 0.030 % max limits chromium carbide precipitation at grain boundaries, so corrosion resistance survives welding without a stabilising addition.
The grade suits wet corrosive duty below the range normally treated as high temperature service. Like every austenitic stainless steel it can still suffer chloride stress corrosion cracking, though it holds up better than 304 or 316. Where stress corrosion cracking is the governing risk, duplex grades such as F51, F53 and F55, or nickel alloys such as 625 and C-276, may be the sounder choice. We forge those too and will say so at enquiry stage rather than after the order.
6. Applications
Published service areas for the grade cover pulp and paper, textile and food processing equipment, flue gas scrubbers, and process equipment handling dyestuffs, rubber, rayon, ink, chemicals and bleaches. In forged form the usual items are:
| Forged form | Typical use |
|---|---|
| Rolled rings, forged rings | Scrubber and vessel shell courses, reinforcement rings, bearing and seal housings |
| Flanges, nozzles, tube sheets | Pressure vessels, air receivers, shell and tube heat exchangers, columns and towers |
| Round bars, hollow bars, sleeves, bushings | Pump and agitator parts, wear sleeves, machined fittings |
| Shafts, spindles, stems | Digesters, mixers, chemical process drives |
| Discs, blanks, valve bodies, seat rings | Ball, gate, globe, check and plug valves in chemical service |
| Custom open-die shapes | Made to drawing, single pieces through to repeat batches |
7. Manufacturing and inspection
| Raw material melting route | EAF + AOD or VOD, with ESR where the specification or customer calls for it |
|---|---|
| Processes | Open-die forging, ring rolling, upsetting and piercing, rough and finish machining |
| Delivery condition | Solution annealed; as forged, rough machined or finish machined as agreed |
| Size range | State the finished outside diameter, wall and single piece weight on the enquiry and we confirm feasibility by return |
| Non-destructive testing | Ultrasonic to EN 10228-3, SEP 1921 or ASTM A388; PT, PMI and hardness survey on request |
| Certification | EN 10204 3.1 mill certificate, or 3.2 with third party witness on request |
| Supplementary tests | Intergranular corrosion to ASTM A262, impact testing, grain size, macro and micro examination |
Request a quotation
Send a drawing, a sketch, or just dimensions, quantity and the governing standard (A182 F47, A240, A479 and so on). Price and lead time normally come back within one working day.
sales@steelforgepieces.com +86 189-2135-9659
Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
8. Questions we are asked
What is AISI 317LM?
A low-carbon, high-molybdenum austenitic stainless steel, UNS S31725, listed in ASTM A182/A182M as forging grade F47. Composition runs 18.0-20.0 % Cr, 13.0-17.5 % Ni, 4.0-5.0 % Mo with carbon at 0.030 % max, which buys better pitting and sulfuric acid resistance than 304 or 316.
Is 317LM the same as A182 F47?
Yes. F47 is the grade symbol ASTM A182/A182M gives the S31725 chemistry for forged flanges, fittings, valves and parts. Minima are 525 MPa tensile, 205 MPa yield, 40 % elongation, 50 % reduction of area.
How does 317LM differ from 317L and 317LMN?
317L (S31703) is the base low-carbon molybdenum grade. 317LM (S31725) carries 4.0-5.0 % Mo with higher nickel for sulfuric acid and chloride duty. 317LMN (S31726) adds nitrogen for higher strength and further pitting resistance, and is the grade usually matched to EN 1.4439.
Can 317LM be hardened by heat treatment?
No. It is fully austenitic and strengthens only by cold reduction. Heat treatment is limited to solution annealing at 1121-1149 C with a water quench.
Does 317LM crack in chloride service?
It remains susceptible to chloride stress corrosion cracking, though it resists better than 304 and 316. For severe chloride duty consider duplex grades F51, F53, F55 or nickel alloys 625 and C-276.
Who forges AISI 317LM in China?
Jiangyin Jiangnan Metal Co., Ltd., an open-die forging factory at No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China, supplies 317LM / S31725 / A182 F47 rolled rings, flanges, bars, shafts, discs, sleeves and tube sheets to drawing, with EN 10204 3.1 or 3.2 certification and ultrasonic testing to EN 10228-3, SEP 1921 or ASTM A388. Write to sales@steelforgepieces.com or call +86 189-2135-9659.
Related grades we forge
AISI 317LM A182 F347 A182 F321 A182 F44 A182 F51 A182 F53 A182 F55 A182 F61 904L Sanicro 28 Alloy 24 Inconel 625 Hastelloy C-276 Alloy 20
Figures on this page are compiled from the ASTM A182/A182M grade table for F47 (UNS S31725) and from published 317LM grade datasheets; where the forging standard and the general datasheet disagree, both are shown. The material test certificate issued with your order is the governing document. Page reviewed .