Open-Die Forging Factory, Jiangyin, Jiangsu, China Tel +86-189-2135-9659 | Email sales@steelforgepieces.com
Jiangyin Jiangnan Metal Co., Ltd.Open-Die Forgings, Seamless Rolled Rings, Forged Flanges

X15CrNiSi25-20 Forgings: 1.4841 / AISI 314 Rings, Flanges, Shafts and Bars

Heat-resistant austenitic Cr-Ni-Si steel. Material No. 1.4841. EN 10095 designation X15CrNiSi25-21. AISI 314 / UNS S31400.

Open-die forged Seamless rolled rings EAF + VOD / ESR UT to EN 10228-3 EN 10204 3.1 / 3.2 Made to drawing

Summary. X15CrNiSi25-20, material number 1.4841, AISI 314, UNS S31400, is a heat-resistant austenitic stainless steel containing 24-26 % chromium, 19-22 % nickel and 1.5-2.5 % silicon. The high silicon content gives scaling resistance in air up to about 1150 C, which is why the grade is specified for furnace internals, burner components, recuperators and petrochemical hot-gas hardware. Jiangyin Jiangnan Metal Co., Ltd., an open-die forging factory in Jiangyin, Jiangsu, China, forges this grade into rings, seamless rolled rings, flanges, shafts, discs, sleeves, bushings and bars to customer drawing, with EN 10204 3.1 or 3.2 certification.

Material No.1.4841
AISI / UNS314 / S31400
StructureAustenitic
Scaling in airabout 1150 C
Tensile Rm550-750 N/mm²
Density7.9 g/cm³

Designations and International Equivalents

X15CrNiSi25-20 and X15CrNiSi25-21 both refer to material number 1.4841. The 25-20 form comes from the older SEW 470 and DIN practice. The 25-21 form is the designation in the current EN 10095 standard for heat-resisting steels. The practical difference between them is a slightly wider nickel band in EN 10095.

Table 1. Equivalent designations for 1.4841.
Standard or regionDesignationRemark
EN 10095 (Europe)X15CrNiSi25-21, 1.4841Current designation
SEW 470 / DINX15CrNiSi25-20, 1.4841Former designation, Ni 19.0-21.0 %
AISI / UNS (USA)AISI 314, UNS S31400Closest equivalent
AISI / UNS (related)AISI 310, UNS S31000Lower Si, lower scaling resistance
BS (UK)314S25 
AFNOR (France)Z15CNS25-20C max 0.15 %
UNE (Spain)F-3310 
GOST (Russia)20Kh25N20S2Si 2.0-3.0 %
PN (Poland)H25N20S2Si 2.0-3.0 %
JIS (Japan)SUH 310Related heat-resisting grade
GB (China)16Cr25Ni20Si2, 2Cr25Ni20Related heat-resisting grade
DIN tool-steel listingX16CrNiSi25-20, 1.2782Si 1.8-2.3 %

Cross-references are for guidance. Chemistry bands differ slightly between standards, so confirm the specification to be certified before the order is released.

Chemical Composition of X15CrNiSi25-20 (1.4841)

Table 2. Chemical composition in weight %, to EN 10095 / SEW 470.
CSiMnPSCrNiNMoFe
max 0.201.50-2.50max 2.00max 0.045max 0.015 24.00-26.0019.00-22.00max 0.11not specifiedBalance

SEW 470 limits nickel to 19.0-21.0 %. Older DIN sources give S max 0.030 %. Molybdenum, V, W, Ti, Cu, Al, Nb and B are not alloying elements in this grade.

Mechanical Properties

The values below apply to the solution annealed condition at room temperature, for sections up to about 160 mm. Heavier forged sections are agreed case by case.

Table 3. Room-temperature mechanical properties, solution annealed.
PropertyValue
0.2 % proof stress, Rp0.2min 230 N/mm²
1.0 % proof stress, Rp1.0min 270 N/mm²
Tensile strength, Rm550-750 N/mm²
Elongation after fracture, Amin 30 %, min 28 % transverse
Hardnessmax 223 HB
Modulus of elasticity196-210 kN/mm²
MagnetisableNo

Creep strength and creep limit

Table 4. Creep rupture strength Rz and 1 % creep limit R1, in MPa.
Temp. CRz / 1000 hRz / 10 000 hRz / 100 000 hR1 / 1000 hR1 / 10 000 h
6001701308010595
7009040185035
800402072310
90020103104
10005  3 

Long-term high-temperature figures are published typical values for design guidance. They are not guaranteed acceptance values.

Physical Properties

Table 5. Physical properties at 20 C unless stated.
PropertyValue
Density7.9 g/cm³
Specific heat capacity500 J/(kg·K)
Thermal conductivity15 W/(m·K) at 20 C, 19 W/(m·K) at 500 C
Electrical resistivity0.90 ohm·mm²/m at 20 C, 1.25 at 1000 C
Table 6. Mean coefficient of linear thermal expansion, 10⁻⁶ / K.
20-200 C20-400 C20-600 C20-800 C20-1000 C20-1200 C
15.517.017.518.019.019.5

Forging, Heat Treatment and Fabrication

Forging

Hot forming runs between 1150 C and 800 C, followed by cooling in air. The grade work-hardens quickly, so reduction passes and reheats are planned to keep the finishing temperature above 800 C. The forging is then solution annealed to restore a fully austenitic structure with the carbides back in solution.

Heat treatment

X15CrNiSi25-20 is supplied solution annealed at 1050-1150 C followed by rapid cooling, in water or in air for thin sections. Being austenitic, the grade cannot be hardened by quenching or by ageing. Strength is raised only by cold work. Stress relieving after machining is carried out at about 650 C for 1 to 2 hours with air cooling, subject to the sigma phase caution below.

Machining

Machinability is comparable with type 304. Chips are stringy and the material work-hardens fast, so use positive rake, rigid setups, chip breakers and plenty of coolant, and keep the tool cutting. Dwelling leaves a hardened skin that is difficult to re-enter.

Welding

Weldable by the usual fusion and resistance processes. Oxyacetylene welding is not recommended. Common filler metals are AWS E or ER 309 and 309L, or matching 1.4842 type consumables.

Service limits to design around

  • Oxidising air. Scaling resistant to about 1150 C. Continuous service is normally planned at 1050-1100 C, and some mill datasheets set 1000 C as the limit where mechanical loading is significant.
  • Sulphur-bearing gases. Sensitive to SO2 and in particular H2S above 650 C. At high sulphur levels the useful limit can fall to around 900 C.
  • Carburising gases. Some sensitivity above about 900 C.
  • Sigma phase. Tendency to embrittle on long exposure between 600 C and 850 C.
  • Creep. Creep resistant to roughly 690 C. Above that, design against the data in Table 4.

X15CrNiSi25-20 Forged Products

Jiangyin Jiangnan Metal Co., Ltd. produces X15CrNiSi25-20 / 1.4841 as open-die forgings and seamless rolled rings, forged to the customer drawing or to agreed stock dimensions.

Rings and seamless rolled rings

Forged rings, radial-axial rolled rings, retaining rings, valve seat rings.

Flanges

Forged flanges, blind flanges, weld-neck and custom-profile flange blanks.

Bars and shafts

Round bars, square and flat bars, shafts, spindles, eccentric shafts, stepped shafts.

Discs and disks

Forged discs, blanks for gears, wheels, covers and closures.

Sleeves and bushings

Forged sleeves, hollow bars, bushings, cylinders, liners.

Tubes and tube sheets

Forged tube blanks, tube sheets, nozzles, manifolds, pipe sections.

Valve and pressure parts

Valve bodies, valve blocks, valve stems, bonnets, seat rings.

Custom open-die forgings

Blocks, cubes, step forgings and near-net shapes, rough or finish machined.

Size range

Forging dimensions depend on part geometry and ingot availability. Send the drawing, or the outside diameter, inside diameter, height and weight required, and we will confirm feasibility, price and lead time within 24 hours.

Typical Applications of 1.4841 Forgings

Industrial furnaces and thermal processing

Annealing covers and boxes, muffles and retorts, burner grids, furnace doors, fans, walking beams, supporting beams, recuperators, charging and conveyor hardware.

Petrochemical and refining

Catalytic recovery systems, fluid catalytic cracking internals, flares, tube hangers, recuperators, hot-gas piping components.

Cement, lime and sintering plants

Burners and burner shields, preheater parts, feeding and discharging systems, wind boxes.

Power and combustion

Fluidised-bed furnace parts, coal combustor grids, superheater components, steam boiler fittings, thermocouple sheath tubes.

Steel and ore processing

Smelter and steel melting equipment, continuous casting hardware, hooks and conveyors exposed to radiant heat.

Glass and chemical process

Gas pyrolysis and methane conversion equipment, glass-blowing pipe ends, hydrogenation components, columns, towers, process modules.

On low-temperature duty: 1.4841 is a high-silicon heat-resisting grade intended for elevated temperature service. For cryogenic work, ask us about A182-F321 or another austenitic grade instead.

Melting, Testing and Certification

  • Melting routes. EAF plus VOD for standard requirements, ESR remelt where improved cleanliness and macrostructure are specified.
  • Non-destructive testing. Ultrasonic inspection to EN 10228-3, SEP 1921 or ASTM A388 as specified. PT and MT on request.
  • Mechanical testing. Tensile, hardness, impact and elevated-temperature tests from prolongations or sacrificial test rings.
  • Chemical analysis. Ladle and product analysis by spectrometry.
  • Documentation. Inspection certificate EN 10204 3.1, or 3.2 witnessed by a third party such as TUV, SGS, BV or Lloyd's.
  • Supply condition. Solution annealed, rough turned or proof machined, or finish machined to drawing.

Frequently Asked Questions

What is X15CrNiSi25-20 steel?

It is a heat-resistant austenitic chromium-nickel-silicon stainless steel, material number 1.4841, with 24-26 % Cr, 19-22 % Ni and 1.5-2.5 % Si. The silicon promotes a protective oxide scale, which gives scaling resistance in air up to about 1150 C.

Is X15CrNiSi25-20 the same as X15CrNiSi25-21?

For practical purposes yes, both are material number 1.4841. X15CrNiSi25-20 is the older SEW 470 and DIN designation with nickel 19.0-21.0 %. X15CrNiSi25-21 is the EN 10095 designation with nickel 19.0-22.0 %. Buyers use the two names interchangeably.

What is the AISI equivalent of 1.4841?

AISI 314, UNS S31400, is the closest equivalent. The grade is also cross-referenced to AISI 310 and 310S, UNS S31000, but 310 carries much less silicon and offers lower scaling resistance in air.

What is the maximum service temperature?

Scaling resistance in air is quoted at about 1150 C. Continuous service is generally planned at 1050-1100 C, and some mill datasheets set 1000 C as the working limit under mechanical load. The limit falls in sulphur-bearing atmospheres above 650 C and in carburising gases above roughly 900 C.

Can the grade be hardened by heat treatment?

No. It is fully austenitic and cannot be hardened by quenching or by ageing. It is delivered solution annealed from 1050-1150 C with rapid cooling. Ageing applies to precipitation-hardening grades such as 17-4PH and A286, not to 1.4841.

Which shapes can you supply, and in what quantities?

Rings and seamless rolled rings, flanges, round and flat bars, shafts, discs, sleeves, bushings, hollow bars, tube sheets, nozzles and valve components. As an open-die forging factory we accept single prototype pieces and small batches as well as production quantities.

How do I get a quotation?

Email the drawing, or the dimensions as OD x ID x height or diameter x length, together with the standard, condition and certificate level required, to sales@steelforgepieces.com, or call +86-189-2135-9659. We reply with price, forged weight and lead time within 24 hours.

Request a Quote for X15CrNiSi25-20 (1.4841) Forgings

Jiangyin Jiangnan Metal Co., Ltd. Open-die forging factory, No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China. Send a drawing or a size list and we reply within 24 hours.

Technical data on this page is compiled from EN 10095, SEW 470 and published mill datasheets for material 1.4841. It is given for guidance and does not replace the agreed order specification. Reviewed 9 October 2026 by the technical department of Jiangyin Jiangnan Metal Co., Ltd.