Heat-resisting austenitic stainless / 25Cr-20Ni
SUS 310S Forgings Rings, seamless rolled rings, flanges, bars, discs, tube sheets and shafts, melted and forged in one works
SUS 310S is the low-carbon member of the 310 family: 24 to 26 percent chromium, 19 to 22 percent nickel, carbon held to 0.08 percent maximum. It holds a stable oxide scale in air to around 1050 C, which is why it ends up in kilns, radiant tubes, retorts, muffles, annealing covers and refinery internals rather than in wet corrosive service.
Jiangyin Jiangnan Metal melts this grade on site. SUS 310S runs through the electric arc furnace, a ladle furnace and vacuum oxygen decarburisation, which is the step that pins carbon under the 0.08 percent ceiling without burning out chromium. It is then forged on the 6,300 t press or rolled on the 6 m ring mill, solution annealed, machined, tested and certified without leaving the plant.
Designations and standards
SUS 310S, 310S, S31008 and 1.4845 all describe the same steel. Buyers hit trouble when a grade name is quoted without a product standard, because plate specifications fix chemistry but say nothing about the forging route or the test location.
| System | Designation | Note |
|---|---|---|
| JIS, Japan | SUS 310S | Bars under JIS G 4303; forgings for pressure vessels fall under JIS G 3214 as SUSF310 |
| ASTM and AISI, USA | 310S | Plate A240, bar A276 and A479, pipe A312, forged flanges and fittings A182 F310 |
| UNS | S31008 | 310 is S31000, 310H is S31009 |
| EN, Europe | 1.4845 | Also written X8CrNi25-21; heat-resisting steels are covered by EN 10095 |
| GB, China | 06Cr25Ni20 | Formerly 0Cr25Ni20 |
| SS, Sweden | 2361 |
For forged flanges, valve parts and fittings in this family the forging specification is ASTM A182 F310. Quoting only the plate specification A240 on a forging order leaves the delivery condition, test prolongation and acceptance criteria undefined. Send the grade and the product standard together and the quotation comes back firm.
Chemical composition
Chromium and nickel are identical across 310, 310S and 310H. Carbon is the only variable that separates them, and it decides where each one can be used.
| Element | SUS 310S / S31008 | 310 / S31000 | 310H / S31009 |
|---|---|---|---|
| Carbon, C | 0.08 max | 0.25 max | 0.04 to 0.10 |
| Manganese, Mn | 2.00 max | 2.00 max | 2.00 max |
| Silicon, Si | 1.50 max | 1.50 max | 0.75 max |
| Phosphorus, P | 0.045 max | 0.045 max | 0.045 max |
| Sulphur, S | 0.030 max | 0.030 max | 0.030 max |
| Chromium, Cr | 24.0 to 26.0 | 24.0 to 26.0 | 24.0 to 26.0 |
| Nickel, Ni | 19.0 to 22.0 | 19.0 to 22.0 | 19.0 to 22.0 |
| Iron, Fe | Balance | Balance | Balance |
Chemistry is verified at the furnace by optical emission spectrometry to ASTM E415, with carbon and sulphur confirmed on an infrared combustion analyser to ASTM E1019. Positive material identification on the finished part is available with a handheld analyser.
Mechanical and physical properties
Those are specification minima for solution-annealed material. On a heavy open-die forging the values that matter are the ones measured on a prolongation or sacrificial ring cut from the piece itself, because section size and sampling position both move the result. The mill certificate carries the tested figures, not the minima.
| Property | Condition | Value |
|---|---|---|
| Density | 8,000 kg/m3 | |
| Modulus of elasticity | 20 C | 200 GPa |
| Shear modulus | 20 C | 77 GPa |
| Poisson ratio | 20 C | 0.30 |
| Thermal conductivity | 100 C | 14.2 W/m.C |
| Coefficient of expansion | 0 to 100 C | 15.9 x 10-6 /C |
| Coefficient of expansion | 0 to 540 C | 17.0 x 10-6 /C |
| Specific heat | 500 J/kg.C | |
| Electrical resistivity | 25 C | 0.78 microhm.m |
| Relative magnetic permeability | 1.02 | |
| Melting range | 1400 to 1450 C |
Published physical data for this grade differs slightly between sources. Density appears as both 8,000 and 7,750 kg/m3, and the melting range is sometimes quoted as 1354 to 1402 C. Where a calculation turns on one of these numbers, take the value from the standard governing the project rather than from a supplier table.
Behaviour at temperature
Grade 310 and 310S resist oxidation in air to approximately 1050 C continuous and 1035 C intermittent. The continuous figure being the higher of the two surprises people, but cyclic heating is what cracks and spalls the protective scale, so steady service is easier on the alloy than repeated heating and cooling.
Those numbers describe clean air. The high chromium with medium nickel gives this grade real capability in reducing sulphur atmospheres containing hydrogen sulphide, where high-nickel alloys struggle, and it is widely used in the moderately carburising conditions found in petrochemical plant. Severely carburising or nitriding service pulls the limit down and points towards Incoloy 800HT, Inconel 601 or Haynes 230. Grade 310 is also a poor choice where parts are repeatedly liquid quenched, because it suffers thermal shock.
At the other end of the scale the same austenitic structure makes 310S useful in cryogenic equipment, where its toughness and low magnetic permeability both count.
Holding 310-series steel between roughly 650 C and 900 C precipitates sigma phase, a hard brittle intermetallic that strips room-temperature ductility and impact toughness. It is reversible: re-solution annealing at about 1040 to 1150 C with rapid cooling puts the sigma back into solution. Operators running 310S through that band commonly schedule a re-anneal between campaigns. Sensitisation, a separate mechanism, happens around 550 to 800 C, and the 0.08 percent carbon cap is what makes 310S more tolerant of it than plain 310.
Where 310S is the wrong material
This is a heat-resisting steel first and a corrosion-resisting steel second. Saying so costs an order occasionally and saves a failure investigation more often.
SUS 310S carries no molybdenum. Despite 25 percent chromium its pitting resistance is poor, and chloride stress corrosion cracking becomes a live risk in chloride-bearing liquids above about 100 C. General corrosion resistance is better than 304, but that is not the same as being suitable for aggressive wet service.
If the duty is driven by pitting, crevice attack or chloride cracking rather than by temperature, the selection should move to 904L, a 6Mo grade such as ASTM A182 F44, or duplex and super duplex grades such as F51, F53 and F55. All of those are forged here, so the enquiry does not need to go elsewhere.
How we melt, forge and treat it
Melting
SUS 310S is melted in the electric arc furnace, refined in the ladle furnace, and decarburised under vacuum in the 30 t or 60 t VOD unit. The vacuum step is the one that matters for this grade: it lets carbon be driven under the 0.08 percent ceiling without oxidising away the chromium that the alloy depends on. Maximum heat size is 60 tonnes. Because the steel is melted here, traceability starts at the melt number rather than at a billet certificate from a third party.
Forging
Working range for 310 and 310S is 975 to 1175 C, with heavy reduction taken down to about 1050 C and only light finishing work below that. Some mills start higher, around 1150 to 1200 C, and finish above 950 C. The alloy is stiff under the hammer compared with 304, so reduction is planned in fewer, heavier bites to keep the piece in its working range. Presses are 6,300 t, 4,000 t and 2,000 t, with 5 t, 3 t, 2 t, 1 t and 750 kg hammers for drawing out and small-batch work. Rings are rolled on 6 m, 3 m and 1 m radial-axial mills, or made by the upset-and-punch route from 50 mm outside diameter upward.
Heat treatment
SUS 310S is supplied solution annealed, typically 1040 to 1065 C soaked through section and cooled rapidly; wider windows of 1030 to 1150 C also appear in the literature. It cannot be hardened by heat treatment and there is no ageing cycle for it. Annealing after forging also relieves forging stress. Because the soak sits above 1000 C, 310S is treated in the high-temperature car-bottom furnaces rather than the standard cars, and that furnace, not the press, is usually what caps the size of a solution-annealed 310S piece. Deep well-type furnaces allow long shafts to be treated and quenched vertically, which keeps them straight.
Machining and welding
Machinability is close to type 304. Work hardening is the nuisance: slow speeds, heavy positive cuts that stay underneath the hardened skin, sharp tooling, generous lubrication and rigid setups. Vertical lathes take 5,000 mm swing, horizontal lathes 14 m between centres, and the deep-hole drilling machine bores 1,600 mm diameter by 10,000 mm.
Welding is straightforward with matching consumables, AWS E310 electrodes or ER310 filler under argon. Preheat and post-heat are not needed. For high-temperature service no post-weld treatment is required beyond thorough slag removal. For any wet corrosive duty, a full post-weld solution anneal plus pickling and passivation is needed to take off the high-temperature oxide and restore the passive film.
SUS 310S forged products and size envelope
Everything is forged to drawing. There is no stock catalogue and no minimum piece count, so a single replacement ring is as quotable as a repeat batch.
| Forged form | Typical service | Size limit and what sets it |
|---|---|---|
| Seamless rolled rings, forged rings, retaining rings | Kilns, radiant tubes, muffles, retorts, annealing covers, furnace rings | OD 50 to 6,000 mm, set by the 6 m radial-axial mill |
| Flanges, tube sheets, discs, covers | Heat exchangers, pressure vessels, air receivers | Up to 5,000 mm machined diameter on the 5,000 mm vertical lathe |
| Shafts, spindles, rolls, eccentric shafts | Furnace rolls, conveyor rollers, fans, gearboxes, compressors | Up to 14,000 mm turned length, with vertical treatment in the well furnaces |
| Hollow cylinders, sleeves, bushings, bored pipe sections | Saggers, oven linings, furnace internals, process modules | Up to 1,600 mm diameter by 10,000 mm on the deep-hole drill |
| Valve bodies, bonnets, stems, seat rings, blocks, nozzles | Gate, globe, ball, check and plug valves in hot gas service | Up to 30,000 kg single piece on the 6,300 t press |
| Round bars, flat bars, blocks, blanks | Refinery FCC internals, machined components, food plant, cryogenic structures | From 10 kg minimum order weight |
Testing, inspection and certification
The works holds CCS, BV, DNV, LR and NK approvals and runs its own laboratory. Standard documentation is an EN 10204 3.1 mill test certificate; 3.2 witnessed by BV, DNV, LR, SGS, TUV or your own inspector is available on request.
| Test | Method | Where it runs |
|---|---|---|
| Chemical analysis | ASTM E415 optical emission, ASTM E1019 carbon and sulphur | On site, at the furnace |
| Positive material identification | Handheld alloy analyser on the finished part | On site |
| Tensile | ASTM A370 or ISO 6892, on prolongation or sacrificial ring | On site |
| Impact | ASTM A370 Charpy V-notch, bath to minus 60 C | On site; below minus 60 C placed with an accredited laboratory |
| Ultrasonic | ASTM A388; EN 10228-4 for austenitic forgings | On site |
| Grain size and metallography | ASTM E112 | On site |
| Intergranular corrosion | ASTM A262 | Accredited third-party laboratory, reported with the certificate |
Purchase specifications regularly call up EN 10228-3 for stainless forgings. That part is written for ferritic and martensitic steel. The part covering austenitic and austenitic-ferritic stainless forgings is EN 10228-4, and that is the one that fits SUS 310S. If your specification names Part 3 for this grade, say so at enquiry stage and the applicable quality class and acceptance criteria can be agreed before the steel is melted rather than argued about at inspection.
Magnetic particle examination to ASTM E709 is available but has no meaning on this grade, since solution-annealed 310S is non-magnetic with a relative permeability near 1.02. Liquid penetrant is the correct surface method for austenitic material.
Questions we get asked
What is SUS 310S equivalent to?
SUS 310S is the JIS name for 25Cr-20Ni heat-resisting austenitic stainless steel. The same material is 310S to ASTM and AISI, S31008 in UNS, 1.4845 in the European material number system, 06Cr25Ni20 in Chinese GB, formerly 0Cr25Ni20, and SS 2361 in Sweden.
What is the difference between 310, 310S and 310H?
Only the carbon. Chromium stays at 24 to 26 percent and nickel at 19 to 22 percent across all three. Grade 310 permits up to 0.25 percent carbon. 310S caps it at 0.08 percent, which makes it the choice where sensitisation or attack by hot gas and condensate is a concern. 310H holds a controlled 0.04 to 0.10 percent band to lift creep strength for pressure service at high temperature.
How hot can SUS 310S run?
About 1050 C continuous and 1035 C intermittent in air. Continuous service tolerates the higher figure because cyclic heating cracks and spalls the protective scale. Sulphur-bearing, low-oxygen, carburising or nitriding atmospheres all reduce the practical limit, and repeated liquid quenching is not recommended because the grade suffers thermal shock.
Can SUS 310S forgings be hardened or age-hardened?
No. It is fully austenitic and has no hardening response to heat treatment, and there is no ageing cycle for it. The delivery condition is solution annealed, commonly 1040 to 1065 C soaked through and cooled rapidly. Only cold work raises strength, which rarely applies to a forging.
What is sigma phase embrittlement and can it be reversed?
Time spent between roughly 650 C and 900 C precipitates sigma phase, a brittle intermetallic that cuts ductility and impact toughness. It is reversible by re-solution annealing at about 1040 to 1150 C with rapid cooling. Plants running 310S through that band often re-anneal between campaigns.
Is SUS 310S any good in seawater or chlorides?
No. There is no molybdenum in it, so pitting resistance is poor, and chloride stress corrosion cracking is a risk above roughly 100 C in chloride-bearing liquid. For those duties look at 904L, a 6Mo grade such as A182 F44, or duplex grades F51, F53 and F55.
Which ultrasonic standard should be specified?
ASTM A388, or EN 10228-4 in the European system, which is the part covering austenitic and austenitic-ferritic stainless forgings. EN 10228-3 applies to ferritic and martensitic forgings. Coarse austenitic grain scatters and attenuates sound, so the technique, probe frequency and acceptance class are worth agreeing before the forging is made.
What is the largest SUS 310S forging you can make?
Rings roll to 6,000 mm outside diameter and the heaviest single piece is 30 tonnes, against a 60 t maximum heat. For 310S the binding constraint is normally the solution-annealing furnace rather than the press, because the soak runs above 1000 C and only the high-temperature cars reach it. Send the dimensions and the treatable size will be confirmed before quoting.
Do you melt the 310S or buy billet?
It is melted here. Electric arc furnace, ladle furnace, then vacuum oxygen decarburisation in the 30 t or 60 t unit, which is what holds carbon under 0.08 percent without stripping chromium. The certificate traces back to the melt number instead of stopping at a purchased billet.
Is there a minimum order, and how long does it take?
Minimum order is 10 kg with no minimum piece count. SUS 310S needs no remelting step, so it sits at the shorter end of the works lead time, normally 20 to 45 days within an overall 20 to 60 day range. Witnessed 3.2 inspection or outside laboratory corrosion testing need scheduling, so flag them with the enquiry rather than after the order.
Request a SUS 310S quotation
Six items give a firm price, usually within two working days: grade or specification, dimensions or a drawing in PDF, DWG, DXF or STEP, quantity and likely repeat volume, delivery condition, heat treatment and testing requirements, and certification plus destination port.