X12CrNi17-7 (EN 1.4310 / AISI 301) Open-Die Forgings

Forged rings, rolled rings, flanges, shafts, discs, sleeves and bars in X12CrNi17-7, made to drawing by Jiangyin Jiangnan Metal Co., Ltd., Jiangyin, Jiangsu, China.

X12CrNi17-7 at a glance

Designation
X12CrNi17-7, the superseded DIN name for EN material number 1.4310. Current EN 10088 steel name is X10CrNi18-8.
Type
Metastable austenitic chromium-nickel stainless steel with a high work-hardening rate
Equivalents
AISI 301, UNS S30100, JIS SUS301, BS 301S21, AFNOR Z11CN18-08, SS 2331
Density
7.9 g/cm³
Annealed strength
Rm 500 to 750 MPa, Rp0.2 195 to 250 MPa, A min. 40 %
Forging
Heat to approx. 1150 to 1200 °C, finish above approx. 930 °C, solution anneal 1000 to 1100 °C and cool rapidly
Supplied by
Jiangyin Jiangnan Metal Co., Ltd. +86-189-2135-9659, sales@steelforgepieces.com

Grade description

X12CrNi17-7 is the older DIN designation for the stainless steel registered under EN material number 1.4310. In the current edition of EN 10088 the grade is named X10CrNi18-8, and mill data sheets for 1.4310 still list X12CrNi17-7 as the previous designation. It is a metastable austenitic Cr-Ni steel, known internationally as AISI 301 and UNS S30100. The main feature of the grade is its high rate of work hardening. Deformation transforms part of the austenite into martensite, so strength rises steeply with cold work while the annealed material stays soft and formable.

Jiangyin Jiangnan Metal Co., Ltd. forges this grade on open-die presses and ring-rolling equipment. Parts are normally supplied solution annealed, with machining allowance or finish machined to the customer drawing.

Note on molybdenum. A number of online listings describe X12CrNi17-7 as a vacuum-remelted austenitic stainless steel alloyed with molybdenum. That description does not match this grade. Molybdenum is not an alloying addition in 1.4310. EN 10088-2 limits it to 0.80 % maximum as a residual element. Where the application calls for a molybdenum-bearing austenitic steel for chloride pitting resistance, specify 1.4401 (316) or 1.4404 (316L) and we will quote those grades.

Chemical composition of X12CrNi17-7 / 1.4310

Composition limits in mass %, to EN 10088-2 for X10CrNi18-8 (1.4310). Elements not listed are not added without agreement with the purchaser.
CSiMnPSCrNiMoN
0.05 to 0.15max 2.00max 2.00max 0.045max 0.015 16.0 to 19.06.0 to 9.5max 0.80max 0.11

The nickel range of 6.0 to 9.5 % is deliberately lean. That is what makes the austenite metastable and gives the grade its work-hardening behaviour. The same leanness affects hot ductility, which is why heating and finishing temperatures are controlled closely during forging.

Mechanical properties

Room-temperature properties for X10CrNi18-8 (1.4310). Annealed values are quoted for nominal diameters 2 to 25 mm. Properties of heavy forged sections are agreed at enquiry and verified on the actual piece.
PropertyConditionValue
Tensile strength RmSoft annealed (+A)500 to 750 MPa
Tensile strength RmSolution annealed and cold drawn (+AT+C)850 to 890 MPa
0.2 % proof strength Rp0.2Soft annealed (+A)195 to 250 MPa
Elongation at fracture ASoft annealed (+A)min. 40 %
Reduction of area ZSoft annealed (+A)60 to 65 %
Brinell hardnessSoft annealed (+A)max 230 HB
DensityNot applicable7.9 g/cm³
Intergranular corrosion resistanceDelivery and sensitised conditionNot resistant

The last line of the table has practical consequences. With carbon permitted up to 0.15 %, 1.4310 sensitises readily, and published data classifies it as not resistant to intergranular corrosion in the as-delivered condition or after sensitisation. For welded assemblies exposed to aggressive media, a low-carbon or stabilised grade such as 1.4541 / 321 or 1.4550 / 347 is the safer selection. We forge both.

Equivalent and comparable grades

Cross-reference for X12CrNi17-7 / 1.4310. Equivalences are close but not always identical. Confirm against the specification governing your order.
Standard or regionDesignation
EN 10088, current nameX10CrNi18-8
EN material number1.4310
DIN Werkstoff, former nameX12CrNi17-7
USA, AISI and UNS301, S30100
Japan, JISSUS301
France, AFNORZ11CN18-08, Z12CN18-09
United Kingdom, BS301S21, 302S26
Sweden, SS2331
ISOX9CrNi18-8

Forging and heat treatment

Published hot-working practice for 1.4310 puts the forging heat at roughly 1150 to 1200 °C, with the stock heated through slowly and evenly rather than charged cold into a hot furnace. Deformation should stop before the section drops below about 930 °C. One data sheet for the same material number gives the forging range as 1150 to 1250 °C, states that the steel must not be forged below 930 °C, and requires solution annealing after forging.

Optimum properties are obtained by solution annealing between 1000 and 1100 °C followed by rapid cooling. Rapid cooling keeps chromium carbides in solution. Slow cooling through the sensitisation range is the condition this carbon level cannot tolerate, so dwelling between roughly 420 and 800 °C is avoided during both heating and cooling.

Heating

Slow, even soak to approx. 1150 to 1200 °C. Avoid dwelling in the 420 to 800 °C band.

Forging

Open-die upsetting, drawing and ring rolling. Finish above approx. 930 °C. Reheat rather than work a chilled section.

Solution anneal

1000 to 1100 °C, then rapid cooling to restore the austenitic structure and corrosion resistance.

X12CrNi17-7 forged product forms

All items below are made to the customer drawing, rough forged, pre-machined or finish machined as required.

Open-die forged product forms available in X12CrNi17-7 / 1.4310.
Product formTypical items
Forged rings and rolled ringsSeamless rolled rings, retaining rings, spacer rings, bearing races, ring blanks
Forged flangesWeld-neck, blind, slip-on, long weld-neck, special profile flanges
Forged shaftsStraight shafts, stepped shafts, spindles, eccentric shafts, crankshafts
Forged discs and disksSolid discs, bored discs, gear and coupling blanks
Forged sleeves and bushingsHollow forgings, liners, bushings, cylinder sleeves
Forged tubes and tube sheetsBored hollow forgings, heat-exchanger tube sheets
Forged bars and blocksRound, square and rectangular bar, step-forged blocks
Forged valve componentsValve bodies, bonnets, stems, seat rings, valve blocks
Forged gear blanksGear blanks, pinion blanks, coupling hubs
Forged nozzles and manifoldsNozzles, hubs, manifold bodies, forging rolls

Applications

The grade is selected where a tough, formable austenitic stainless steel with good general corrosion resistance and high strength after working is wanted, and where the service environment does not demand a molybdenum-bearing or stabilised grade. Common component groups include chemical and food-processing equipment, pressure vessel and heat-exchanger internals, columns, towers, tanks and silos, general mechanical and power-transmission parts, and valve and pump components. Since the steel is not rated for intergranular corrosion resistance after sensitisation, welded parts in corrosive duty should be checked against alternative grades before the order is placed. We will review the selection with you at enquiry stage.

Testing, inspection and certification

X12CrNi17-7 forgings can be supplied with ultrasonic examination to EN 10228-3, SEP 1921 or ASTM A388 as agreed, together with chemical analysis, mechanical testing and dimensional inspection. Material certificates are issued to EN 10204 3.1, or to EN 10204 3.2 with third-party endorsement where the specification calls for it. State the acceptance class and the inspection body at enquiry stage, since both affect lead time and price.

Frequently asked questions

Is X12CrNi17-7 the same material as 1.4310?

Yes. X12CrNi17-7 is the superseded designation for material number 1.4310. The current EN 10088 steel name for the same material number is X10CrNi18-8. Drawings and older specifications still use X12CrNi17-7, and we accept orders under either name.

Does X12CrNi17-7 contain molybdenum?

Not as an alloying addition. EN 10088-2 permits a maximum of 0.80 % Mo as a residual element. Descriptions of this grade as molybdenum-alloyed are inaccurate.

What is the forging temperature for X12CrNi17-7?

Approximately 1150 to 1200 °C, with forging stopped before the section cools below about 930 °C, followed by solution annealing at 1000 to 1100 °C and rapid cooling.

Can X12CrNi17-7 be welded?

It can be welded, but carbon up to 0.15 % makes it prone to sensitisation, and the grade is not classified as resistant to intergranular corrosion in the delivery or sensitised condition. For welded parts in corrosive service a low-carbon or stabilised austenitic grade is usually preferred.

What sizes and weights can you forge?

Capacity depends on the product form. Send the drawing, or the rough dimensions and finished weight, and we will confirm feasibility against our press and ring-rolling capacity before quoting.

How are X12CrNi17-7 forgings priced?

Open-die forgings are quoted individually against the drawing. Price depends on finished weight, machining state, heat treatment, non-destructive testing and certification level, so no list price applies to this grade.

Who supplies X12CrNi17-7 forgings?

Jiangyin Jiangnan Metal Co., Ltd., an open-die forging factory at No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province 214423, China, makes X12CrNi17-7 forged rings, flanges, shafts, discs, sleeves, tube sheets and bars to drawing. Contact sales@steelforgepieces.com or +86-189-2135-9659.

Request a quotation for X12CrNi17-7 forgings

Send the drawing, or the grade, dimensions, quantity and certification required. We reply with price, lead time and, where useful, a comment on whether X12CrNi17-7 suits the duty.

Company
Jiangyin Jiangnan Metal Co., Ltd., open-die forging factory
Address
No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province 214423, China
Phone and WhatsApp
+86-189-2135-9659
Email
sales@steelforgepieces.com
Please include
Grade, product form, dimensions, quantity, heat-treatment condition, NDT requirement and certificate type (EN 10204 3.1 or 3.2)

Email an enquiry

Related stainless steel forging grades

If X12CrNi17-7 is not the right fit, these grades cover adjacent requirements: 17-7PH and 17-4PH for precipitation-hardened high strength, A182-F321 and A182-F347 for stabilised weldable austenitics, A182-F51, A182-F53 and A182-F55 for duplex and super duplex, 904L and Sanicro 28 for high-alloy corrosion service, and Nitronic 60 for galling resistance.

Technical sources

  1. EN 10088-1, 10088-2 and 10088-3 data for X10CrNi18-8 (1.4310): composition, mechanical properties and equivalent grades, European Steel and Alloy Grades database (steelnumber.com).
  2. thyssenkrupp Materials (UK) data sheet for stainless steel 1.4310 / 301, which records X10CrNi18-8 as the material code and X12CrNi17-7 as the previous designation.
  3. Swiss Steel Group data sheet for 1.4310: solution annealing range and sensitisation behaviour.
  4. Zapp Ergste 1.4310 data sheet: forging temperature range and minimum finishing temperature.

Values are given for guidance. The governing document for any order is the purchase specification agreed in writing.

Last updated . Published by Jiangyin Jiangnan Metal Co., Ltd., open-die forging manufacturer, Jiangyin, Jiangsu, China.