Home / Stainless Steel / 904L

904L Forgings, UNS N08904 / EN 1.4539, to ASTM A182 F904L

Rolled rings, flanges, discs, shafts, bars, sleeves and tube sheets, forged from our own melt and supplied solution annealed.

904L is a low carbon, high alloy austenitic stainless steel running about 20 % chromium, 25 % nickel, 4.5 % molybdenum and 1.5 % copper. The copper is what separates it from 316L: it carries the alloy through sulphuric and other reducing acids. The nickel and molybdenum handle chloride pitting, crevice attack and stress corrosion cracking. Buyers who order by UNS number will see the same alloy listed as UNS N08904.

UNS
N08904
EN number
1.4539
Forging spec
ASTM A182 F904L
Tensile min
490 MPa
Yield 0.2 % min
215 MPa
Elongation min
35 %

Designations

Table 1. The same alloy across the main standards
StandardDesignation
UNSN08904
Common trade name904L
ASTM forgingsA182 / A182M Grade F904L
EN material number1.4539
EN designationX1NiCrMoCu25-20-5

The EN 1.4539 chemistry window is drawn slightly tighter than the ASTM window. Confirm which specification governs the order before the melt is booked.

Chemical composition

Table 2. ASTM A182 / A182M Grade F904L, weight percent
ElementContent
Carbon0.02 max
Manganese2.00 max
Phosphorus0.04 max
Sulphur0.03 max
Silicon1.00 max
Chromium19.00 to 23.00
Nickel23.00 to 28.00
Molybdenum4.00 to 5.00
Copper1.00 to 2.00
IronBalance

Carbon is held at 0.02 % maximum. That is low enough to keep chromium carbides off the grain boundaries during welding, which is why the grade carries no stabilising addition and why the L suffix is part of the name.

Mechanical properties

Acceptance values for forgings

Table 3. ASTM A182 F904L, room temperature, solution annealed
PropertyMinimum
Tensile strength490 MPa (71 ksi)
Yield strength, 0.2 % offset215 MPa (31 ksi)
Elongation in 50 mm (2 in.) or 4D35 %

Flat rolled product to ASTM B625 is listed at 220 MPa minimum yield and about 150 HB. Those figures are often quoted for 904L generally, but forgings are accepted against the A182 values above.

Physical properties

Table 4. Typical values at room temperature
PropertyValue
Density7 900 kg/m³
Modulus of elasticity190 GPa
Thermal expansion, 0 to 100 °C15 µm/m·°C
Thermal conductivity11.5 W/m·K
Specific heat, 0 to 100 °C500 J/kg·K
Electrical resistivity952 nΩ·m
Magnetic responseNon-magnetic, annealed

Corrosion behaviour

Reducing acids

The copper addition is the reason the grade exists. It gives resistance to sulphuric acid and phosphoric acid, and this is where 904L earns its cost against 316L.

Chlorides

Resistant to pitting and crevice corrosion in chloride bearing media, which covers seawater cooling and ballast service.

Stress corrosion cracking

The 23 to 28 % nickel gives resistance to chloride stress corrosion cracking, the failure mode that limits 304 and 316 in hot chloride service.

Where it is weaker

In aggressive nitric acid it performs worse than molybdenum free grades such as 304L and 310L. It is a corrosion grade, not a high temperature structural grade.

Table 5. Pitting resistance equivalent, PREN = %Cr + 3.3×%Mo + 16×%N
AlloyUNSPREN
Nitronic 50S2091034
904LN0890435
Duplex 2205S3180336
Super duplex 2507S3275041 to 43

PREN is calculated from composition and predicts chloride pitting only. It says nothing about acid service, which is the reason 904L is specified in the first place. Published 904L figures sit between 34 and 36 depending on the heat analysis used.

Choosing between grades

Duplex 2205 reaches a similar PREN at higher strength and lower alloy cost, and on that basis it has taken over a good deal of work that once went to 904L. The case for 904L holds where reducing acids are present, since duplex gains nothing from copper, and where the service temperature rules duplex out. If chloride pitting alone is the problem and the budget allows, a 6 % molybdenum super austenitic or a super duplex is the step up.

Forging and heat treatment

Melting

904L is melted here on the EF, LF and VOD route. The VIM, VAR and protective atmosphere ESR routes are available where cleanliness requirements go beyond the standard.

Hot working

Forged between 850 and 1150 °C. Deformation is not continued below roughly 950 °C because the alloy work hardens fast and the cracking risk climbs. Fully austenitic grades need more press load than carbon steel at the same temperature, which is one reason section size and reduction are planned before the first heat.

Solution treatment

Hot work is followed by solution annealing and a rapid quench. Published ranges run from 1050 to 1175 °C depending on the governing specification, so the order dictates the figure used. Cooling speed through the sensitising band matters more than the soak temperature. A slow cool undoes the corrosion resistance the material was bought for. 904L does not respond to hardening heat treatment; it takes strength from cold work only.

Welding

Welded by the usual processes with no preheat and no post weld heat treatment. ER385 to AWS A5.9 is the normal filler. The alloy solidifies fully austenitic and is therefore sensitive to hot cracking in restrained joints, so heat input and joint design need watching. Annealing after fabrication is not usually necessary, but it is worth doing where the part will see severe stress corrosion cracking conditions.

Surface condition

Parts leave pickled. Scale and embedded iron from handling break down the passive film, so the pickling step is not cosmetic.

Product forms

Table 6. 904L forged forms and where they go
FormTypical service
Seamless rolled ringsAcid plant, pump and valve bodies, bearing and seal housings
Flanges, weld neck, slip on, blindChemical, refinery and offshore pipework
Shafts and spindlesSeawater pumps, agitators, crystalliser drives
Round bar and blocksValve stems, seat rings, machined components
Discs and blanksPump and compressor internals, closures
Sleeves, bushings, hollowsLiners, wear sleeves, down-hole parts
Tube sheets and nozzlesHeat exchangers, scrubbers, pressure vessels

End markets are sulphuric, phosphoric and acetic acid plant, fertiliser production, oil refining, offshore and seawater systems, desalination, pulp and paper, flue gas scrubbing, and pharmaceutical and food processing.

Size range

Table 7. Working envelope, set by plant equipment
ItemLimitSet by
Seamless rolled ringsOD 50 to 6,000 mm6 m radial axial ring mill
Shafts, turned lengthup to 14,000 mmC61160 lathe; 15 m well furnace for vertical quench
Discs, tube sheets, blocksup to 5,000 mm5,000 mm vertical lathe
Bored cylinders and hollows1,600 mm dia x 10,000 mmCNC deep hole drilling machine
Single piece weightup to 30,000 kg60 t heat size; 6,300 t press
Minimum order10 kgNo minimum piece count
Lead time20 to 60 daysGrade and testing scope

The works

Jiangyin Jiangnan Metal Co., Ltd. has operated in Zhouzhuang Town, Jiangyin City since 1997. The plant melts its own steel rather than buying billet, so a 904L order is traceable from the melt number through to the shipped part without leaving the site.

Melting runs on EF, LF and VOD for carbon, alloy, stainless and duplex grades, with VIM, VAR and protective atmosphere ESR for clean and superalloy work, to a maximum heat size of 60 tonnes. Forging is on presses of 6,300, 4,000 and 2,000 tonnes with 6 m, 3 m and 1 m radial axial ring mills, backed by 14 heat treatment furnaces and an in-house machine shop. The payroll is 460 people, including 9 senior engineers, 32 intermediate engineers and 140 technicians.

The works holds CCS, BV, DNV, LR and NK approvals and ships to North America, Europe, the Middle East and Asia-Pacific.

Testing and documents

Table 8. Standard scope, extended on request
ItemStandard
Ultrasonic testingASTM A388, EN 10228-3 or SEP 1921, class to order
Chemical analysisOptical emission spectrometry to ASTM E415, PMI on request
Mechanical testingTensile to ASTM A370; hardness; impact on request
Intergranular corrosionASTM A262 or ASTM G28, accredited third party laboratory
Pitting resistanceASTM G48, accredited third party laboratory
CertificateEN 10204 3.1 standard, EN 10204 3.2 witnessed on request

Questions we are asked

Is UNS N08904 the same as 904L?

Yes, one alloy and two names. UNS N08904 is the Unified Numbering System entry, 904L is the trade name, EN 1.4539 and X1NiCrMoCu25-20-5 are the European designations, and forgings are bought to ASTM A182 F904L.

Is 904L a stainless steel or a nickel alloy?

A stainless steel. Iron is still the base element. With 23 to 28 % nickel it sits at the boundary of the nickel alloy family, which is why it is priced closer to them than to 316L.

Is 904L magnetic?

No. It is fully austenitic and non-magnetic in the solution annealed condition.

What is the PREN of 904L?

About 35. Figures between 34 and 36 appear in the literature depending on the heat analysis. Duplex 2205 is at a similar level and super duplex 2507 is higher.

Can it be used hot?

It has useful oxidation resistance, but it is specified for corrosion service, not as a high temperature structural grade. Service temperature limits should be taken from the governing design code for the vessel or line.

What do you need to quote?

A drawing, or the rough dimensions and quantity, plus the governing specification, the certificate level and the UT class. State whether the part is wanted black as forged, proof machined, or finish machined.

Request a quotation

904L forgings are quoted against a drawing or a written specification rather than sold from a price list. Send the dimensions and we will come back with price and lead time, normally within two working days.

Works No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
Phone 0086-189-2135-9659
Email sales@steelforgepieces.com

Related grades