AISI 301 Stainless Steel (UNS S30100): Data Sheet and Made-to-Order Forgings

Grade reference and forging capability from Jiangyin Jiangnan Metal Co., Ltd., an open-die forging factory in Jiangyin, Jiangsu, China.

AISI 301 (UNS S30100, EN 1.4310, JIS SUS 301) is a 17% chromium, 7% nickel austenitic stainless steel. It contains no molybdenum. The grade work-hardens very fast, gaining roughly 14 MPa of strength for every 1% reduction in area of cold work, so cold-rolled 301 reaches a higher strength than any other 300-series stainless.

For that reason 301 is normally supplied as strip, sheet and wire for springs, clips and formed structural parts. It is not a common forging grade. ASTM A240 and ASTM A666 cover flat-rolled product, and ASTM A182 contains no F-designation for 301. We forge 301 rings, bars and discs to order, and we will say so when 304, 316 or 17-7 PH is a better fit for a forged part.

Chemical composition

The limits below are the composition requirements for Type 301 in ASTM A240 / ASME SA240 and ASTM A666. Values are maximum unless a range is shown, in weight percent.

Table 1. AISI 301 (UNS S30100) composition limits, wt%
CMnSiPSCrNiNMoFe
0.15 max2.00 max1.00 max0.045 max0.030 max16.0 to 18.06.0 to 8.00.10 maxnone specifiedbalance

Note on older data. Some published data sheets for this grade list a molybdenum content and give ASTM A182 as the governing standard. Both are wrong. Type 301 is a plain chromium-nickel austenitic steel with no Mo requirement. A drawing that calls for molybdenum usually points to A182 F316 or a 6% Mo grade such as A182 F44.

Low-carbon and nitrogen variants

Only Type 301 itself is specified in ASTM A666. Grade 301L is the low-carbon version, 0.03% C max with nitrogen up to 0.20%, covered by JIS G4305 and used where better ductility is needed. Grade 301LN is EN 10088-2 grade 1.4318, 16.5 to 18.5% Cr with 0.10 to 0.20% N, and work-hardens even faster than standard 301. Neither 301L nor 301LN needs post-weld annealing to restore corrosion resistance. Standard 301 does.

Mechanical properties

Annealed 301 has the highest stretch formability of any stainless steel. Heavily cold-worked 301 has the highest strength of any 300-series stainless. The annealed figures below are ASTM A240 / SA240 minima. The temper figures are ASTM A666 minima for cold-worked flat-rolled product.

Table 2. Specified minimum room-temperature properties
ConditionTensile strength, minYield strength 0.2%, minElongation in 50 mm, minHardness, max
Annealed (A240)515 MPa (75 ksi)205 MPa (30 ksi)40%95 HRB
1/4 hard (A666)862 MPa (125 ksi)517 MPa (75 ksi)25%not specified
1/2 hard (A666)1034 MPa (150 ksi)758 MPa (110 ksi)15 to 18%not specified
3/4 hard (A666)1205 MPa (175 ksi)930 MPa (135 ksi)10 to 12%not specified
Full hard (A666)1276 MPa (185 ksi)965 MPa (140 ksi)8 to 9%not specified

Elongation ranges cover the two thickness bands in ASTM A666, below and at or above 0.015 in. Tensile strength up to about 1800 MPa is reported for heavily cold-worked 301 strip and wire, above the specified temper minima. Published annealed elongation minima differ between sources, 40% under A240 against 60% quoted elsewhere for annealed A666 strip, so check the exact edition and product form named on your order.

Physical properties

Table 3. Typical physical properties
PropertyValue
Density7880 kg/m3 (0.285 lb/in3)
Modulus of elasticity193 GPa (28.0 x 10^6 psi)
Mean thermal expansion, 0 to 100 C16.9 um/m.C
Mean thermal expansion, 0 to 315 C17.2 um/m.C
Mean thermal expansion, 0 to 538 C18.2 um/m.C
Thermal conductivity at 100 C16.2 W/m.K
Thermal conductivity at 500 C21.4 W/m.K
Specific heat, 0 to 100 C500 J/kg.K
Electrical resistivity695 nOhm.m
Magnetic responseNon-magnetic annealed, magnetic after cold work

Grade equivalents

Table 4. Approximate international equivalents for AISI 301
AISI/SAEUNSEN numberEN nameOld British BSSwedish SSJIS
301S301001.4310X10CrNi18-8301S212331SUS 301

These grades are functionally similar rather than identical. National standards differ on carbon, nitrogen and residual limits, so a 301 equivalent certificate is not automatically acceptable to a customer ordering to ASTM.

Corrosion and heat resistance

Corrosion resistance is close to 304 and adequate in mildly corrosive conditions at ambient temperature, but lower than 304/304L. The 0.15% carbon ceiling leaves 301 open to carbide precipitation during welding, which is why 304L is specified instead on many welded assemblies. In oxidising service 301 resists oxidation intermittently to about 840 C and continuously to about 900 C. Oxidation resistance is not strength retention. 301 is not a creep-resistant grade and should not be selected for sustained load at high temperature.

Heat treatment, forming and welding

Annealing

Solution anneal at 1010 to 1120 C and cool rapidly. A lower range is used for intermediate annealing between cold-working passes. 301 cannot be hardened by heat treatment. All of its high strength comes from cold work.

Cold working and machining

The work-hardening rate is about 14 MPa per 1% reduction in area, and strained austenite partly transforms to martensite. That is where the strength comes from, and it is also why the material stiffens under a tool. Machinability is poorer than free-machining grades. Use positive rake, a rigid setup and a heavy constant feed, and do not let the tool dwell. Enough ductility remains at high strength levels for severe cold deformation.

Welding

All standard processes are suitable, with 308L filler metal. Welded parts in standard 301 should be annealed afterwards for full corrosion resistance, which also removes the strength gained by cold rolling. Spot welding is the usual method for assembling cold-rolled 301 components and does not reduce overall strength. 301L and 301LN need no post-weld anneal.

Forging

301 is forged hot, above the strain-hardening range, then solution annealed and cooled rapidly. We set the forging and annealing window per order against the certified analysis of the heat and the section size, rather than publishing one figure for every job. Ask for the route sheet before you place the order.

Where AISI 301 is used

Documented uses for 301 are high-strength formed and spring parts rather than pressure-containing forgings: rail car structural components, airframe sections, highway trailer components, automotive wheel covers, wiper blade clips and holders, stove element clips, screen frames, toaster springs and architectural curtain walls. Precision springs in compression, extension, torsion and flat forms are the largest single use of 301 strip. Tempers from 3/4 hard to full hard are also used for wear resistance in simple formed shapes.

Buyers looking for forged flanges, valve bodies, tube sheets or wellhead parts are usually on the wrong grade. Those items normally go out in A182 F316, F51 or F53 duplex, F44, or 17-4 PH. Send us the application and we will quote the grade that will pass your inspection.

Forged product forms in AISI 301

Every item is made to order from your drawing or dimensions. We hold no 301 forging stock, and there is no list price: each enquiry is quoted on weight, machining allowance and test requirements.

  • Seamless rolled rings and forged rings
  • Forged flanges
  • Round bars, blocks and billets
  • Discs, blanks and blank gears
  • Shafts, spindles and stepped shafts
  • Sleeves, bushings and hollow bars
  • Forged tube and pipe sections
  • Near-net open-die shapes

Testing and certification

Ultrasonic examination to EN 10228-3, SEP 1921 or ASTM A388 as your order requires, with certification to EN 10204 3.1, or 3.2 under third-party witness. Chemical analysis, tensile, hardness and grain-size reporting are available on request. State the acceptance class in the enquiry so it is priced in from the start.

Choosing between 301 and the alternatives

Table 5. When to move off 301
AlternativeReason to use it instead
304 and 304LA lower work-hardening rate is acceptable and better forming ductility is wanted. 304L suits welded assemblies because the lower carbon avoids carbide precipitation.
316Higher corrosion resistance is required and the lower work-hardening rate can be designed around.
301L and 301LN301 strength character with better ductility (301L), or an even higher work-hardening rate (301LN).
17-7 PH and 17-4 PHHigh strength is needed in a thick forged section, where cold work cannot deliver it and a heat-treatable precipitation-hardening grade is the correct route.

Frequently asked questions

Does AISI 301 contain molybdenum?

No. AISI 301 (UNS S30100) is a 17% chromium, 7% nickel austenitic stainless steel, and the composition tables in ASTM A240 and ASTM A666 specify no molybdenum for it. Data sheets that list a Mo content for 301 have taken the figure from another alloy.

Which standard covers AISI 301?

ASTM A240 / ASME SA240 and ASTM A666 for flat-rolled product, plus the aerospace specifications AMS 5901 annealed, AMS 5517 quarter hard, AMS 5518 half hard, AMS 5902 three-quarter hard and AMS 5519 full hard. ASTM A182, which covers forged flanges and fittings under F-designations, does not include Type 301.

Is AISI 301 stronger than 304?

Annealed, the two are close. Cold worked, 301 is much stronger, because it gains about 14 MPa for each 1% reduction in area and reaches full-hard minima of 1276 MPa tensile and 965 MPa yield under ASTM A666. The cost is lower corrosion resistance than 304 and much lower elongation in the hard tempers.

Is AISI 301 magnetic?

It is non-magnetic in the annealed condition and becomes magnetic after cold working, because strained austenite partly transforms to martensite.

Can AISI 301 be hardened by heat treatment?

No. Thermal hardening does not apply to this grade. Strength is developed by cold rolling or roll forming. Solution annealing at 1010 to 1120 C with rapid cooling softens it again.

Can you supply AISI 301 as forgings?

Yes, to order. Jiangyin Jiangnan Metal Co., Ltd. forges AISI 301 rings, bars, discs, shafts and sleeves from customer drawings, with ultrasonic examination to EN 10228-3, SEP 1921 or ASTM A388 and certification to EN 10204 3.1 or 3.2. Since 301 is mainly a strip and wire grade, we review the application first and may recommend 304, 316 or a precipitation-hardening grade instead. Contact sales@steelforgepieces.com or +86 189 2135 9659.

What is the European and Japanese equivalent of AISI 301?

Approximately EN 1.4310 (X10CrNi18-8), JIS SUS 301, old British 301S21 and Swedish SS 2331. These are functionally similar rather than exact equivalents, so check the original specification before substituting.

Sources and limits of this data

Composition, temper, physical property and equivalence figures on this page follow published summaries of ASTM A240 / SA240 and ASTM A666, including AZoM, Stainless Steel Grade 301 (UNS S30100) and Rolled Metal Products, Type 301. They are given for information only. Do not use them as design or acceptance criteria in place of the current edition of the governing standard and the mill test report for your heat.

Request a quotation for AISI 301 forgings

Send a drawing or finished dimensions, quantity, specification and test requirements. You get a price and a lead time from the factory, not from a trading desk.

Jiangyin Jiangnan Metal Co., Ltd., Open-Die Forging Factory
No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China

Email sales@steelforgepieces.com Call +86 189 2135 9659