1.4910 / X3CrNiMoBN17-13-3 Forgings: Bars, Rolled Rings, Discs, Shafts, Flanges and Hollow Sections
Austenitic creep-resisting stainless steel, closest equivalent AISI 316LN / UNS S31653. Forged from steel melted in our own works, to 6,000 mm outside diameter and 30 t single-piece weight.
1.4910 is an austenitic creep-resisting chromium-nickel-molybdenum stainless steel alloyed with nitrogen and boron. It is designated X3CrNiMoBN17-13-3 in EN 10302 and EN 10088-1, and X3CrNiMoN17-13-3 in EN 10222-5, the standard for steel forgings for pressure purposes. Nominal composition is max 0.04 % C, 16.0 to 18.0 % Cr, 12.0 to 14.0 % Ni, 2.0 to 3.0 % Mo, 0.10 to 0.18 % N and 0.0015 to 0.0050 % B. Density is about 7.98 to 8.0 g/cm³. The closest American equivalent is AISI 316LN / UNS S31653. In practice the grade is the high-temperature version of 1.4429: the boron addition raises creep resistance and slows grain growth during long exposure at temperature.
Jiangyin Jiangnan Metal Co., Ltd. forges 1.4910 to customer drawing at No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China. The works melts its own steel on a 25 t electric arc furnace with 25 t and 50 t ladle furnaces and 30 t and 60 t vacuum oxygen decarburisation, maximum heat size 60 tonnes. Forging runs on 6,300 t, 4,000 t and 2,000 t presses, rings roll to 6,000 mm outside diameter, and heat treatment, machining and testing all stay on site. Minimum order is 10 kg, quotations come back in two working days, lead time is 20 to 60 days, and EN 10204 3.1 certification is standard with 3.2 on request. Contact sales@steelforgepieces.com or +86 189 2135 9659.
Largest rolled ring
6 m radial-axial mill, with 3 m and 1 m mills for smaller rings.
Heaviest single forging
Worked under a 6,300 t hydraulic open-die press. Maximum heat size 60 t.
Minimum order
No minimum piece count. A single part is quotable.
Traceability
From melt number to shipped part, not from a purchased billet certificate.
Designations and supply basis
| EN material number | 1.4910 |
|---|---|
| EN name, EN 10302 and EN 10088-1 | X3CrNiMoBN17-13-3 |
| EN name, EN 10222-5 forgings | X3CrNiMoN17-13-3 |
| Closest AISI and UNS equivalent | AISI 316LN, UNS S31653. Cross-reference only, see equivalents |
| Classification | Austenitic creep-resisting steel |
| Alloy system | 17Cr, 13Ni, 3Mo, nitrogen and boron alloyed |
| Density | 7.98 to 8.0 g/cm³, about 0.289 lb/in³ |
| Usual delivery condition | +AT solution annealed. +A soft annealed also available |
| Forged forms from this works | Round, square, flat and hex bars. Hollow bars, sleeves, bushings, cylinders, housings, hubs, forged pipe sections. Seamless rolled rings and forged rings. Discs, blocks, plates, tube sheets. Shafts, spindles, flanges |
| Certification | EN 10204 3.1 standard, EN 10204 3.2 witnessed on request |
| Manufacturer | Jiangyin Jiangnan Metal Co., Ltd., Jiangyin City, Jiangsu Province, China, established 1997 |
What the grade is, and why the boron is there
1.4910 belongs to the same 17Cr, 13Ni, 3Mo family as 316L and 316LN, but the European standards list it as a creep-resisting steel rather than a general corrosion-resisting one. Two additions cause that. Nitrogen at 0.10 to 0.18 % strengthens the austenite in solution, which is why the certified proof strength stays useful well above room temperature. Boron at 0.0015 to 0.0050 %, a range narrow enough that it has to be aimed at during refining rather than corrected afterwards, improves long-term creep resistance and slows grain growth at temperature.
The result is a steel that behaves like 1.4429 or 316LN in a corrosive environment but holds up better when the environment is hot and the load is carried for years. European suppliers describe it as the high-temperature version of 1.4429. It is the grade designers reach for when a 316-type austenitic is wanted for boiler and pressure-vessel duty, and it is the one listed in EN 10269 for elevated-temperature bolting.
The 0.04 % carbon ceiling also keeps it resistant to intergranular corrosion in the sensitised condition according to EN 10028-7. EN 10216-5 takes a different position on that point for seamless tube, so if intergranular attack matters to your design, state the standard and the test on the enquiry rather than relying on a general claim.
Chemical composition
| C | Si | Mn | P | S | Cr | Mo | Ni | N | B | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| 0.04 | 0.75 | 2.00 | 0.035 | 0.015 | 16.0 to 18.0 | 2.0 to 3.0 | 12.0 to 14.0 | 0.10 to 0.18 | 0.0015 to 0.0050 | balance |
Boron identifies this grade. A specified boron range is uncommon among wrought stainless steels, and it is what separates 1.4910 from 1.4429. Pitting resistance equivalent calculated from the nominal composition is roughly 27.
Mechanical properties at room temperature
| Property | +A soft annealed | +AT solution annealed |
|---|---|---|
| Tensile strength Rm | 550 to 780 MPa | 550 to 750 MPa |
| 0.2 % proof strength Rp0.2 | 260 to 300 MPa | min 260 MPa |
| Elongation A, longitudinal | 35 to 40 % | min 35 % |
| Elongation A, transverse | 35 to 40 % | min 40 % |
| Charpy KV at +20 C, longitudinal | min 100 J | min 120 J |
| Charpy KV at +20 C, transverse | min 60 J | min 80 J |
Typical values published for the solution annealed condition, for comparison rather than acceptance: Brinell hardness about 200 HB, elongation at break about 41 %, Charpy V-notch about 98 J, fatigue strength about 250 MPa, shear strength about 450 MPa, Poisson's ratio 0.28. Acceptance is always against the standard invoked on the order, tested on a piece representing the forging.
Proof strength at elevated temperature, condition +AT
| Temperature C | 50 | 100 | 150 | 200 | 250 | 300 | 350 | 400 | 450 | 500 | 550 | 600 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Rp0.2 min, MPa | 234 | 205 | 187 | 170 | 159 | 148 | 141 | 134 | 130 | 127 | 124 | 121 |
The curve flattens above about 400 C, which is the point of the nitrogen addition. More than 45 % of the room-temperature proof strength is still there at 600 C. Scale resistance in air is given as 700 C. For sustained service, design against the creep-rupture data in EN 10302 rather than against short-term proof strength.
Physical properties
| Density | 7.98 to 8.0 g/cm³ |
|---|---|
| Modulus of elasticity E | 198 to 200 GPa, about 29 x 106 psi |
| Shear modulus G | about 78 GPa |
| Specific heat capacity | 450 to 470 J/kg·K |
| Thermal conductivity | 16 W/m·K |
| Electrical resistivity | 0.77 ohm·mm²/m |
| Coefficient of linear expansion | 16.3 to 18.7 x 10-6 /K |
| Magnetic response | Austenitic, essentially non-magnetic in the solution annealed condition |
| Scale resistance in air | up to about 700 C |
| Melting range | about 1400 to 1440 C |
Standards that list 1.4910
| Standard | Scope | Relevance to forgings |
|---|---|---|
| EN 10222-5 | Steel forgings for pressure purposes, martensitic, austenitic and austenitic-ferritic stainless steels | The main forging specification. The grade is named X3CrNiMoN17-13-3 here. |
| EN 10302 | Creep resisting steels, nickel and cobalt alloys, bar, rod and flat products | Source of the chemistry and the creep data. The standard that classes 1.4910 as creep-resisting. |
| EN 10028-7 | Flat products of steels for pressure purposes, stainless steels | Plate equivalence, and the source of the intergranular corrosion position. |
| EN 10216-5 | Seamless steel tubes for pressure purposes, stainless steel tubes | Relevant where forged hollow sections meet tube. |
| EN 10269 | Steels and nickel alloys for fasteners with specified elevated and low temperature properties | The bolting route: stud bolts and threaded components. |
| EN 10088-1 | Stainless steels, list of stainless steels | Registers the designation X3CrNiMoBN17-13-3 against number 1.4910. |
Give the standard, the edition and the delivery condition on your enquiry. The same material number carries different test frequencies, orientations and acceptance values depending on whether it is ordered to EN 10222-5, EN 10302 or EN 10269, and the certificate has to match the design code the part is registered under.
Equivalent and related designations
| System | Designation | Status |
|---|---|---|
| EN number | 1.4910 | Exact |
| EN name | X3CrNiMoBN17-13-3 | Exact, EN 10302 and EN 10088-1 |
| EN name | X3CrNiMoN17-13-3 | Exact, EN 10222-5 name for the same number |
| Trade short form | X3CrNiMoN17-13 | Common with European stockholders |
| AISI / SAE | 316LN | Closest equivalent, no boron requirement |
| UNS | S31653 | Closest equivalent, no boron requirement |
| Related EN grade | 1.4429, X2CrNiMoN17-13-3 | The stainless counterpart without boron. 1.4910 is its high-temperature version |
| Welding consumable | 1.4430 type filler | Suggested filler. Qualify the procedure for the application |
Treat 316LN and S31653 as cross-references, not substitutions. UNS S31653 corresponds most directly to 1.4429, and because 1.4910 additionally specifies boron, a certificate reading S31653 does not on its own demonstrate compliance with 1.4910. If your drawing calls for 1.4910 and a local supplier offers 316LN, check which specification the acceptance criteria are written against before approving the change. We quote either, and we state which one the certificate will read.
Forging, heat treatment and machining
| Forging and rolling temperature | 1200 C down to 900 C |
|---|---|
| Annealing and solution annealing | 1020 to 1100 C |
| Cooling after solution treatment | Rapid, fast enough to avoid carbide and nitride precipitation through the sensitising range |
| Hardening by heat treatment | Not applicable. Austenitic, strengthened by nitrogen in solution and by cold work |
| Weldability | Described as excellent. Filler of the 1.4430 type, procedure to be qualified |
| Machinability | As for nitrogen-alloyed austenitics. Work-hardens readily, so use rigid setups, positive rake, generous feed and flood coolant |
Two process points decide whether a 1.4910 forging certifies. The first is the finish-forging temperature. Stop too high and the grain coarsens, which shows up in the transverse Charpy result before it shows up anywhere else. The second is the cooling rate out of solution treatment, which sets the proof strength and the sensitisation behaviour. Both are furnace-chart items on our route sheet, and both charts go out with the certificate.
On heavy sections the reduction ratio and the proof-machining stage are planned together, so that ultrasonic testing to ASTM A388 or EN 10228-3 is done on a surface that can be read, not on as-forged scale.
Applications and industries
1.4910 is specified where a 316-type austenitic is needed and the service is hot as well as corrosive. Published applications include pressure vessels and steam boilers, boiler components and installation parts, superheaters, steam piping and headers, heat exchangers and tube sheets, turbine and machine components, and elevated-temperature fasteners such as stud bolts and threaded bars under EN 10269. The buying industries are power generation, chemical and petrochemical processing, pressure equipment and boiler manufacturing, and heavy engineering.
Power generation
Boiler and superheater components, casing and header flanges, turbine parts, heat-exchanger tube sheets.
Chemical and petrochemical
Pressure-vessel flanges, covers, tube sheets, pump and valve parts for hot corrosive duty.
Pressure equipment
Forgings ordered to EN 10222-5 with EN 10204 3.1 or witnessed 3.2 certification.
Elevated-temperature bolting
Forged bar stock for stud bolts and threaded components to EN 10269.
Forged product forms and size envelope
Everything below is forged from a single piece of steel melted at this works. No welding, no casting, no purchased billet of unknown origin. Full equipment list on the works overview.
| Product form | Typical items | Size limit and what sets it |
|---|---|---|
| Seamless rolled rings | Rectangular and contoured section rings, gear ring blanks, slewing rings, bearing races | 50 mm to 6,000 mm outside diameter. 6 m, 3 m and 1 m radial-axial ring mills |
| Forged rings | Upset and punched rings, retaining rings, valve seat rings | Sections outside the ring-mill envelope, heavy reduction route |
| Forged bars and blocks | Round, flat, square and hexagonal bars, blocks, billets, slabs | 6,300 t, 4,000 t and 2,000 t presses, 5 t to 750 kg hammers |
| Hollow bars, sleeves, cylinders, pipe sections | Bushings, bushes, barrels, casings, shells, hubs, housings, couplings | Bored to 1,600 x 10,000 mm on the CNC deep-hole drilling machine |
| Discs, blocks, plates, tube sheets | Solid forged discs, blanks, covers, tube sheets, proof-machined for UT | Up to 5,000 mm machined on the 5,000 mm swing vertical lathe |
| Shafts and spindles | Stepped, gear, pinion and eccentric shafts, spindles, rotors, tie rods | Up to 14,000 mm turned length. 15 m well furnaces for vertical quench |
| Flanges | Weld neck, blind, slip-on, socket weld, lap joint, orifice, long weld neck | To ASME B16.5, B16.47, MSS SP-44 or drawing |
| Single-piece weight | Up to 30,000 kg. 60 t maximum heat size, 6,300 t press | |
Why in-house melting matters for this grade
1.4910 is defined by two elements present in small, tightly bounded amounts: nitrogen at 0.10 to 0.18 % and boron at 0.0015 to 0.0050 %. Both have to be hit during refining. A forging shop that buys billet inherits whatever nitrogen and boron the billet supplier achieved, and can only verify it after the fact.
This works melts its own steel. Stainless and duplex grades run through a 25 t electric arc furnace, are refined in 25 t and 50 t ladle furnaces and decarburised in 30 t and 60 t vacuum oxygen decarburisation units, the route used where low carbon and close nitrogen control are needed. Where extra cleanliness is wanted on a nitrogen-alloyed grade, 3 t and 6 t protective-atmosphere electroslag remelting is available on site. Maximum heat size is 60 tonnes.
- Chemistry aimed at the forging it will become, rather than accepted as delivered.
- The certificate traces the part back to its melt number, not to a purchased billet certificate.
- Melt shop, presses, ring mills, 14 heat-treatment furnaces, machine shop and laboratory on one site, with no subcontracted forging, heat treatment or machining step.
- 460 staff, including 9 senior engineers, 32 intermediate engineers and 140 technicians. Technical questions are answered by an engineer on site.
Testing, approvals and certification
The works holds CCS, BV, DNV, LR and NK approvals and runs its own laboratory. Because the steel is melted here, chemistry is verified at the furnace instead of being copied from a supplier certificate.
| Test | Method or standard | Where performed |
|---|---|---|
| Chemical analysis | Optical emission spectrometry, ASTM E415 | In-house |
| Carbon and sulphur | Infrared analyser, ASTM E1019 | In-house |
| Positive material identification | Handheld alloy analyser | In-house |
| Tensile | ASTM A370, ISO 6892. 600 kN and 300 kN machines | In-house |
| Charpy V-notch impact | ASTM A370, down to -60 C | In-house |
| Ultrasonic testing | ASTM A388, EN 10228-3 | In-house |
| Magnetic particle | ASTM E709 | In-house |
| Grain size and metallography | ASTM E112 | In-house |
| Intergranular corrosion | ASTM A262 or ASTM G28 | Accredited third-party laboratory |
| Pitting resistance | ASTM G48 | Accredited third-party laboratory |
| Impact below -60 C, bench Brinell and Rockwell | As specified | Accredited third-party laboratory |
EN 10204 3.1 mill test certificates are supplied as standard. EN 10204 3.2 witnessed by BV, DNV, LR, SGS, TUV or your own inspector is available on request. Heat-treatment charts, NDT reports, dimensional reports and PMI records go with the certificate. ASTM A262 is placed outside, so state it at enquiry stage and it is scheduled before shipment instead of being added afterwards.
Request a quotation
A price comes back within two working days from a complete enquiry. Minimum order is 10 kg with no minimum piece count. Normal lead time is 20 to 60 days by material route. Send these six items and no round trip of questions is needed.
| # | Item | Example |
|---|---|---|
| 1 | Grade and specification, with edition | 1.4910 to EN 10222-5, condition +AT |
| 2 | Dimensions, or a drawing in PDF, DWG, DXF or STEP | OD 1200 x ID 900 x H 260 mm rolled ring |
| 3 | Quantity and expected repeat volume | 12 pcs, about 4 times per year |
| 4 | Delivery condition | Proof-machined for UT |
| 5 | Heat treatment and testing | Solution annealed, UT to EN 10228-3, ASTM A262 Practice E |
| 6 | Certification and destination | EN 10204 3.2 witnessed by DNV, Rotterdam |
Email a pre-filled 1.4910 enquiry Call, WhatsApp or WeChat +86 189 2135 9659
Jiangyin Jiangnan Metal Co., Ltd. No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China, 214423. Monday to Saturday, 08:00 to 17:30 China Standard Time, UTC+8. English and Chinese. Made to order from your drawing or specification. Not a stockist and not a trading company. Further details on the contact page.
Frequently asked questions
What is 1.4910 stainless steel?
An austenitic creep-resisting chromium-nickel-molybdenum stainless steel alloyed with nitrogen and boron. It is designated X3CrNiMoBN17-13-3 in EN 10302 and EN 10088-1, and X3CrNiMoN17-13-3 in EN 10222-5. Nominal chemistry is max 0.04 % C, 16.0 to 18.0 % Cr, 12.0 to 14.0 % Ni, 2.0 to 3.0 % Mo, 0.10 to 0.18 % N and 0.0015 to 0.0050 % B. Nitrogen raises strength, boron improves long-term creep resistance and slows grain growth at temperature.
What is the difference between 1.4910, 316LN and 1.4429?
All three are nitrogen-alloyed austenitics of the 17Cr, 13Ni, 3Mo type, and 1.4910 is routinely cross-referenced to AISI 316LN and UNS S31653. The distinguishing feature is boron. 1.4910 specifies 0.0015 to 0.0050 % B, which raises creep resistance and long-term strength at temperature. That is why 1.4910, and not 1.4429, appears in EN 10302 and in EN 10269 for elevated-temperature fasteners. A certificate to S31653 does not by itself prove compliance with 1.4910.
Which standards cover 1.4910?
EN 10302 for creep resisting steels, nickel and cobalt alloys. EN 10222-5 for steel forgings for pressure purposes, stainless steels. EN 10028-7 for flat products for pressure purposes. EN 10216-5 for seamless tubes for pressure purposes. EN 10269 for fasteners with specified elevated and low temperature properties. EN 10088-1, the list of stainless steels.
What are the mechanical properties of 1.4910 forgings?
Solution annealed, +AT: tensile strength 550 to 750 MPa, 0.2 % proof strength minimum 260 MPa, elongation minimum 35 % longitudinal and 40 % transverse, Charpy KV at +20 C minimum 120 J longitudinal and 80 J transverse. Soft annealed, +A: tensile strength 550 to 780 MPa, proof strength 260 to 300 MPa, elongation 35 to 40 %, KV at +20 C 100 J longitudinal and 60 J transverse. Minimum proof strength falls from 234 MPa at 50 C to 121 MPa at 600 C.
At what temperature is 1.4910 forged and heat treated?
Forging and rolling run between 1200 C and 900 C. Annealing is at 1020 to 1100 C followed by rapid cooling. Finish-forging temperature governs grain size and therefore transverse impact energy. Cooling rate out of solution treatment governs proof strength and sensitisation behaviour. Both are recorded on furnace charts issued with the certificate.
Which 1.4910 forged products can Jiangyin Jiangnan Metal supply?
Round, square, flat and hexagonal forged bars. Hollow bars, sleeves, bushings, bushes, cylinders, barrels, casings, shells, hubs, housings and forged pipe sections. Seamless rolled rings and forged rings. Discs, blocks, plates and tube sheets. Shafts, spindles and flanges. Rings roll from 50 mm to 6,000 mm outside diameter, the heaviest single forging is 30 tonnes, shafts turn to 14,000 mm, discs machine to 5,000 mm and bores run to 1,600 x 10,000 mm. Minimum order 10 kg, no minimum piece count.
Do you melt 1.4910 yourselves, or buy billet?
We melt it. Stainless and duplex grades run through a 25 t electric arc furnace, 25 t and 50 t ladle furnaces and 30 t and 60 t vacuum oxygen decarburisation units, the route used where low carbon and close nitrogen control are needed. Protective-atmosphere electroslag remelting at 3 t and 6 t is available for nitrogen-alloyed grades needing extra cleanliness. Maximum heat size is 60 tonnes, and traceability starts at the melt number rather than at a purchased billet.
What certification comes with 1.4910 forgings?
EN 10204 3.1 mill test certificates as standard, EN 10204 3.2 witnessed by BV, DNV, LR, SGS, TUV or your own inspector on request. The works holds CCS, BV, DNV, LR and NK approvals. In-house testing covers spectrometry, PMI, tensile, Charpy to -60 C, UT, MT and metallography. ASTM A262, G28, G48 and impact below -60 C are placed with an accredited third-party laboratory and reported alongside the mill certificate.
What is the lead time and minimum order?
Lead time is 20 to 60 days from order confirmation depending on the material route, with standard stainless grades at the lower end and grades needing a remelting step at the upper end. Minimum order is 10 kg with no minimum piece count. Witnessed 3.2 inspection and outside corrosion testing need scheduling, so flag them at enquiry stage to have them built into the quoted date.
Is 1.4910 resistant to intergranular corrosion?
EN 10028-7 records 1.4910 as resistant to intergranular corrosion in the delivery condition and in the sensitised condition, which follows from the 0.04 % carbon ceiling. EN 10216-5 takes a different position for seamless tube. Where intergranular attack matters to the design, nominate the standard and the acceptance test, for example ASTM A262 Practice E, on the order.
Related grades we forge
Data sources
Composition and mechanical data are stated to EN 10302:2008 and EN 10222-5 and cross-checked against published grade datasheets. The values are standard limits, not guaranteed properties of a particular forging. Acceptance values for your order are those of the standard and edition invoked on the purchase order, certified on a test piece representing the forging.
- EN 10302:2008, Creep resisting steels, nickel and cobalt alloys. Chemistry and mechanical limits for X3CrNiMoBN17-13-3, number 1.4910.
- EN 10222-5, Steel forgings for pressure purposes, Part 5, martensitic, austenitic and austenitic-ferritic stainless steels. Designation X3CrNiMoN17-13-3.
- EN 10088-1, EN 10028-7, EN 10216-5 and EN 10269. Further standards listing material number 1.4910.
- Published grade datasheets for 1.4910, AISI 316LN and UNS S31653 for physical properties, processing temperatures and equivalence cross-references.