Jiangyin Jiangnan Metal Co., Ltd. Open-die forging factory, Jiangsu, China +86 189 2135 9659 sales@steelforgepieces.com
Jiangnan MetalOpen-die forging & ring rolling, since 1997 Get a quote

Grade datasheet for open-die forgings and seamless rolled rings

1.4466 X1CrNiMoN25-22-2

Fully austenitic urea-grade stainless steel, nominally 25 Cr / 22 Ni / 2 Mo with 0.10–0.16 % nitrogen and carbon held below 0.020 %.

EN steel name
X1CrNiMoN25-22-2
EN / Werkstoff no.
1.4466
UNS
S31050
ASTM / ASME forgings
A182 / SA-182 F310MoLN
Common name
310MoLN
China GB/T
022Cr25Ni22Mo2N
ISO 15510:2014
4466-310-50-E
France AFNOR
Z1 CND 25.22 Az

1.4466 (X1CrNiMoN25-22-2, UNS S31050, ASTM A182 Grade F310MoLN) is a fully austenitic, nitrogen-alloyed, extra-low-carbon 25Cr–22Ni–2Mo stainless steel developed for the high-pressure section of urea plants, where it resists ammonium carbamate corrosion. Jiangyin Jiangnan Metal forges it into rings, flanges, tube sheets, discs and valve parts up to 6,000 mm outside diameter and 30 tonnes, melted in-house on the EAF + VOD route, supplied solution annealed and water quenched with EN 10204 3.1 or witnessed 3.2 certification.

§01 What 1.4466 is, and what it is for

Grade record

Structure
Fully austenitic. Ferrite content very low to zero; urea licensors commonly cap δ-ferrite on the finished part.
Nominal chemistry
25 Cr, 22 Ni, 2.1 Mo, 0.12 N, C ≤ 0.020 %
Primary EN standard
EN 10088-3 (bars, rods, sections, semi-finished products)
Primary ASTM standard
ASTM A182/A182M Grade F310MoLN
Delivery condition
Solution annealed and quenched (+AT)
PREN
≈ 34
Service temperature
−50 to +400 °C for bar and forgings in pressure service under VdTÜV-Wbl 415/3; austenitic toughness extends far lower
Page revised

The grade was developed to survive ammonium carbamate, the intermediate that forms when ammonia and carbon dioxide react on the way to urea. Carbamate at 180–210 °C and 130–150 bar attacks ordinary austenitic stainless steel quickly, and it attacks grain boundaries first. Three features of the composition deal with that.

  • Chromium at 24–26 % builds and rebuilds the passive film that carbamate strips away, and gives the grade its resistance to hot concentrated nitric acid as well.
  • Carbon held at or below 0.020 % leaves almost nothing to form chromium carbides at grain boundaries, so the steel stays resistant to intergranular attack both as delivered and after sensitising exposure.
  • Nitrogen at 0.10–0.16 % replaces the strength that the missing carbon would have given, and stabilises austenite so that a 25 % chromium alloy stays fully austenitic instead of forming the ferrite that duplex grades rely on. Ferrite is not wanted in carbamate service.

Molybdenum at 2 % adds pitting and crevice resistance. The resulting pitting resistance equivalent is roughly 34, which puts the grade close to 904L in chloride service.

A correction worth reading before you order

1.4466 is sometimes described as an austenitic-ferritic (duplex) steel containing 25–28 % Cr, 4.5–6.5 % Ni and 1.3–2.0 % Mo, with a tensile strength of 880 MPa and solution annealing at 950–1000 °C. That description has circulated on supplier pages, including an earlier version of this one.

Those composition figures belong to a different steel: 1.4460, X3CrNiMoN27-5-2, which is a genuine austenitic-ferritic grade. Its EN 10088-3 tensile band is 620–880 MPa, so 880 MPa is the top of that range rather than a minimum for anything. 1.4466 is fully austenitic, carries about 22 % nickel, and its EN 10088-3 tensile band in the solution annealed condition is 540–740 MPa. No heat of 1.4466 will reach 880 MPa in the delivery condition, and a solution anneal at 950–1000 °C is far too cold for it. If a specification you have been given quotes those values against 1.4466, the grade reference and the property table disagree, and the order needs clarifying before anything is melted.

§02 Designations, equivalents and governing standards

The same steel is sold under at least a dozen names. They are not all interchangeable on paper: composition limits differ slightly between EN and ASTM, so a purchase order should name both the specification and the number.

Cross-reference for 1.4466
SystemDesignationNotes
EN steel nameX1CrNiMoN25-22-2EN 10088-1/-2/-3
EN steel number1.4466Werkstoffnummer
UNSS31050United States
ASTM / ASME forgingsA182 F310MoLN / SA-182 F310MoLNThe grade to quote for ASME code forgings
ASTM tube and pipeA213 / A312, UNS S31050Seamless tube and pipe
Common trade name310MoLNLow-carbon, molybdenum and nitrogen version of 310
ISO 15510:20144466-310-50-EISO numbering
China GB/T022Cr25Ni22Mo2NISC S31053
France AFNORZ1 CND 25.22 AzSuperseded by EN
Producer names2RE69, Ultra 725LN, A405, UREA 310Mo LNAlleima (formerly Sandvik), Outokumpu, voestalpine BÖHLER, Industeel
Close but different1.4465 (X1CrNiMoN25-25-2)25Cr–25Ni–2Mo, a separate SEW 400 grade; do not substitute without approval

Sources: EN 10088-1/-2/-3 grade listings; ISO 15510:2014; producer datasheets [1] [2] [3] [4].

Where the grade is standardised

1.4466 appears in EN 10088-1, EN 10088-2, EN 10088-3, EN 10088-4, EN 10088-5, EN 10028-7, EN 10216-5, EN 10297-2 and EN 13445-2, as well as ISO 15510 and ISO 9328-7. For pressure equipment it also carries VdTÜV-Werkstoffblatt 415, 415-2 and 415-3 approvals, and S31050 is approved under the ASME Boiler and Pressure Vessel Code Section VIII Divisions 1 and 2, with ASME Code Case 2038-5 covering forgings. Cite the revision number: earlier revisions of Code Case 2038 cover tube and pipe rather than forgings.

For forged products specifically: EN 10088-3 is the material standard usually cited for bars, semi-finished products and open-die forgings in Europe; ASTM A182 Grade F310MoLN is the specification to cite for flanges, fittings and valve parts in ASME-code work. There is no dedicated EN forging part for this grade, so European enquiries normally read EN 10088-3 X1CrNiMoN25-22-2 (1.4466), solution annealed with the testing and delivery requirements written out separately.

§03 Chemical composition

EN and ASTM limits for this grade are close but not identical, with silicon and molybdenum differing most, so the governing specification has to be stated on the order. We melt to whichever applies, and can hold tighter internal ranges where a licensor specification demands it.

Chemical composition, mass %, iron balance
Element EN 10088-3 / -2
X1CrNiMoN25-22-2
ASTM A182 F310MoLN
as published by BÖHLER for A405
Typical producer analysis
Alleima 2RE69, nominal
Carbon, C≤ 0.020≤ 0.030≤ 0.020
Silicon, Si≤ 0.70≤ 0.40≤ 0.4
Manganese, Mn≤ 2.00≤ 2.001.7
Phosphorus, P≤ 0.025≤ 0.030≤ 0.015
Sulfur, S≤ 0.010≤ 0.015≤ 0.010
Chromium, Cr24.0 – 26.024.0 – 26.025
Nickel, Ni21.0 – 23.021.0 – 23.022
Molybdenum, Mo2.00 – 2.502.00 – 3.002.1
Nitrogen, N0.10 – 0.160.10 – 0.160.12

Sources: EN 10088-2:2005 and EN 10088-3:2014 composition tables [1] [2]; voestalpine BÖHLER A405 datasheet, stated as related to ASTM A182 [3]; Alleima 2RE69 datasheet [4]. Elements not listed are not to be added intentionally without the purchaser's agreement.

Why the melting route matters for this grade

Carbon below 0.020 % and nitrogen inside a 0.06 % window are difficult to hit together in an open furnace: blowing carbon out normally takes nitrogen with it, and re-nitriding overshoots. Vacuum oxygen decarburisation solves this by decarburising at reduced pressure and then trimming nitrogen under control. Our melt shop runs a 25 t electric arc furnace, 25 t and 50 t ladle furnaces and 30 t and 60 t VOD units, so 1.4466 is melted and refined here rather than bought in as billet of unknown history. The certificate traces back to the melt number, not to a purchased bar.

§04 Mechanical properties

All values below are for the solution annealed and quenched condition (+AT). Like every fully austenitic stainless steel, 1.4466 has a low proof strength relative to its tensile strength, and very high ductility. It is specified for corrosion resistance, so pressure parts made from it are correspondingly thick.

EN 10088-3:2014, bars, rods, sections and bright products, condition +AT
Diameter or thickness Tensile strength Rm Proof strength Rp0.2 Elongation A Impact KV2 Hardness
d ≤ 160 mm 540 – 740 MPa≥ 250 MPa≥ 35 % (long.)≥ 100 J (long.)≤ 240 HBW
160 < d ≤ 250 mm 540 – 740 MPa≥ 250 MPa≥ 30 % (tr.)≥ 60 J (tr.)≤ 240 HBW

Source: DIN EN 10088-3:2014 property table for X1CrNiMoN25-22-2 [2]. long. = longitudinal, tr. = transverse.

ASTM A182/A182M Grade F310MoLN (UNS S31050), solution treated and quenched
PropertyMetricImperial
Tensile strength, min540 MPa78 ksi
Yield strength 0.2 %, min255 MPa37 ksi
Elongation in 50 mm or 4D, min25 %25 %
Reduction of area, min40 %40 %
HardnessNo A182 limit for this gradeProducer figure: max 95 HRB

Source: ASTM A182 mechanical requirements table for F310MoLN / S31050 [5]. A182 sets no hardness limit on this grade; the 95 HRB figure is Alleima's own maximum for 2RE69 [4] and the 240 HBW ceiling above is EN's. Always confirm against the edition of A182 named in your purchase order.

Strength at elevated temperature

Minimum proof and tensile values fall steadily with temperature. The table below is the producer data published for seamless tube and pipe, which sits on a higher room-temperature basis than the EN bar minima above it; lower values may apply to bar, plate and forgings, so design figures for a forged part should be agreed against the applicable code table rather than taken from tube data.

Minimum strength at temperature (Alleima 2RE69, tube and pipe)
TemperatureRp0.2 minRp1.0 minRm min
50 °C250 MPa285 MPa555 MPa
100 °C230 MPa260 MPa530 MPa
150 °C215 MPa245 MPa510 MPa
200 °C200 MPa230 MPa500 MPa
250 °C190 MPa215 MPa490 MPa
300 °C175 MPa205 MPa480 MPa
350 °C165 MPa195 MPa470 MPa
400 °C155 MPa185 MPa460 MPa
450 °C145 MPa175 MPa455 MPa
500 °C140 MPa170 MPa450 MPa

Source: Alleima 2RE69 material datasheet [4].

Toughness at low temperature

Austenite has no ductile-to-brittle transition, so 1.4466 keeps its toughness far below zero. Producer testing on this grade meets EN 13445-2 (minimum 60 J at −270 °C) and EN 10216-5 (minimum 60 J at −196 °C). For pressure equipment in bar and forged form, VdTÜV-Wbl 415/3 covers the grade from −50 °C to +400 °C; the flat-product sheet runs from −195 °C. Our pendulum machine with its cooling bath covers Charpy testing down to −60 °C in house; colder test temperatures are placed with an accredited laboratory and reported alongside the mill certificate.

§05 Physical properties

Thermal conductivity is roughly a third that of carbon steel, and thermal expansion is about half again as high. Both figures affect fabrication: welding distortion and thermal stress have to be planned for in the weld sequence.

Physical properties, solution annealed condition
Property20 °C100 °C200 °C300 °C400 °C500 °C
Modulus of elasticity, GPa195190182174166158
Thermal conductivity, W/m·K131517192123
Specific heat, J/kg·K485505540565585605
Mean expansion from 30 °C, ×10⁻⁶/Kn/a15.516.016.517.017.0
Room-temperature constants
PropertyValueNote
Density7.9 g/cm³ (0.29 lb/in³)EN 10088 tabulates 8.0 g/cm³ for this grade
Electrical resistivity≈ 0.80 Ω·mm²/mAt 20 °C
Relative magnetic permeability1.003At 6,400–55,700 A/m, effectively non-magnetic
MachinabilityMediumReduce carbide cutting speeds by about 30 % for finishing and 60 % for roughing against 316L

Sources: Alleima 2RE69 datasheet [4]; EN 10088 grade data [1] [2]; European stockist data for 1.4466 [6].

§06 Forging and heat treatment practice

Hot working

Forge between 1,150 °C and 850 °C. Below 850 °C the alloy work-hardens sharply and surface cracking risk rises, so heavy sections are reheated rather than pushed. Every forging is solution annealed afterwards, because hot working alone does not leave the microstructure the grade needs.

Solution annealing

1,070–1,150 °C, held long enough for the section to reach temperature, then quenched rapidly in water. Producer practice for thin sections is 1,070–1,120 °C for 5–15 minutes; heavy forged sections take the upper part of the range and a longer soak.

If the order is to ASTM A182, the standard sets its own solution-treatment range for F310MoLN, around 1,050–1,100 °C with a liquid quench, which is narrower than the EN and producer range above. A forging annealed at 1,150 °C would then be outside the specification, so confirm the figure against the edition of A182 named in your order and we will treat to it.

Why the quench has to be fast

With carbon at 0.020 % there is little carbide to worry about, but a 25 Cr–2 Mo austenite will precipitate sigma and chi phases if it dwells around 600–900 °C. Those phases take toughness and carbamate resistance with them. On large rings and tube sheets the cooling rate is usually limited by section thickness rather than by the furnace setting.

After welding

Post-weld heat treatment is normally not required, and the grade resists intergranular corrosion after welding without it. Where residual stress is a concern, or where a licensor requires it, a full solution anneal and quench is the correct treatment. A stress-relief soak in the precipitation range is not.

Sources: Alleima 2RE69 heat treatment and hot bending data [4]; European stockist thermal treatment data for 1.4466 [6]; voestalpine BÖHLER A405 [3].

Our heat treatment capacity. Fourteen furnaces on site, including car-bottom chambers to 8,000 × 2,000 × 2,000 mm, two 15 m deep well-type furnaces that let long shafts hang vertically through the quench, and three high-temperature car-bottom furnaces. Solution annealing and quenching of 1.4466 is done here, with charts kept and issued with the certificate. Nothing is subcontracted.

§07 Corrosion performance

Pitting resistance equivalent

PREN is calculated from the composition using the nitrogen-weighted formula. On the nominal analysis:

PREN = %Cr + 3.3 × %Mo + 16 × %N
= 25.0 + 3.3 × 2.1 + 16 × 0.12
= 25.0 + 6.93 + 1.92 = 33.85

BÖHLER states PREN > 33 for the grade and Outokumpu lists 34 for its equivalent. That places 1.4466 above 316L and close to 904L for chloride pitting, though chloride resistance is a by-product here rather than the design target.

Ammonium carbamate and urea service

The longest producer service record in a urea stripper stands at 35 years, and the alloy is written into the high-pressure material lists of the major urea process licensors, including Stamicarbon, Saipem, Kellogg and Urea Casale. Carbamate resistance depends on passivation air being present in the process; where a licensor's design removes or reduces passivation air, the material choice needs revisiting with them.

Intergranular corrosion

EN 10088 records the grade as resistant to intergranular corrosion both in the delivery condition and in the sensitised condition, and BÖHLER states resistance to intergranular corrosion up to 400 °C. In the Huey test (boiling 65 % nitric acid, ASTM A262 Practice C), producer data for straight tube in the as-delivered condition gives a guaranteed maximum of 0.12 mm/year with selective attack guaranteed below 20 µm and typically under 10 µm. Urea licensor specifications usually set their own Huey limits and a maximum selective attack depth; state them on the enquiry so the test is scheduled before shipment.

Nitric acid, pitting, crevice and stress corrosion

  • Nitric acid. High chromium with very low carbon gives excellent resistance across a wide range of concentration and temperature, which is why the grade also appears in nitric acid cooler-condensers on polluted cooling water and in NPK plant heating coils.
  • Pitting and crevice. Critical pitting temperature in neutral chloride solution is well above that of 316L, and crevice resistance is considerably better.
  • Stress corrosion cracking. The higher nickel content makes 1.4466 somewhat more resistant than 304 or 316 in chloride solutions, but it is not immune. Chlorides carried in boiler feed water or process steam remain a credible SCC risk and should be controlled rather than designed around.
  • Erosion corrosion. The combination of strength and passivity is why ferrules at stripper tube inlets are made from this grade.

Delta-ferrite

The grade is designed to be free of ferrite, and producers report very low to zero ferrite content. Urea licensors frequently impose a ceiling on δ-ferrite in the finished component, and a limit at or below 0.5 FN is not unusual on stripper and reactor parts. No standard imposes that limit, so it has to be written into the order. It then constrains heat selection at the melt shop as well as the final inspection.

Sources: Alleima 2RE69 corrosion data, Huey and CPT results [4]; voestalpine BÖHLER A405 product description [3]; EN 10088 grade notes [1].

§08 Welding

Weldability is good, and the practice is conventional for a fully austenitic grade. The one point that needs attention is heat: low thermal conductivity and high expansion mean input has to be limited and distortion allowed for when the weld sequence is set.

Recommended welding practice
ItemRecommendation
Preferred processesGTAW/TIG as first choice; GMAW/MIG; SMAW/MMA with covered electrodes
Filler, GTAW / GMAWISO 14343 S 25 22 2 N L
Filler, SMAWISO 3581 E 25 22 2 N L B
Overlay of tube sheets and vesselsISO 14343 S 25 22 2 N L wire or strip
PreheatNone
Heat input< 1.0 kJ/mm
Interpass temperature< 100 °C
TechniqueString beads rather than weaving
Post-weld heat treatmentNormally none; solution anneal and quench if residual stress must be removed

Source: Alleima 2RE69 welding recommendations [4]. Confirm consumables against your own WPS and the licensor specification.

§09 Where 1.4466 is used

Urea plants, high-pressure section

  • Stripper tube sheets, shells and ferrules
  • Carbamate condenser components
  • Reactor internals and reactor coils
  • High-pressure carbamate piping fittings, flanges and valve parts
  • Decomposers and separators

Nitric acid and fertilizer

  • Nitric acid cooler-condensers, including polluted cooling water duty
  • Heating coils and pipe in NPK plants
  • Absorber and acid-handling components

Other duties

  • Chemical and petrochemical plant where hot chlorides and oxidising acids meet
  • Cryogenic components, on the strength of austenitic low-temperature toughness
  • Pressure equipment built to EN 13445 or ASME VIII where the grade is code approved

Sources: producer application lists and urea licensor material specifications [3] [4].

§10 What we forge in 1.4466

Every item is forged from a single piece of steel melted on this site, with no welding, no casting and no purchased billet. The size limits below are the plant's envelope. On a given part the practical limit is usually set by the heat-treatment furnace or the lathe rather than by the press.

Working envelope for 1.4466 forgings
LimitValueSet by
Maximum ring outside diameter6,000 mm6 m radial-axial ring rolling mill
Minimum ring outside diameter50 mmUpset-and-punch route below ring-mill range
Maximum single-piece weight30,000 kg60 t heat size and 6,300 t press
Maximum machined disc diameter5,000 mmØ5,000 mm vertical turning lathe
Maximum turned shaft length14,000 mmC61160 horizontal lathe
Maximum bored lengthØ1,600 × 10,000 mmCNC deep-hole drilling machine
Minimum order10 kgNo minimum piece count

Production route for a 1.4466 forging

  1. Melt and refine. Electric arc furnace, ladle furnace, then vacuum oxygen decarburisation to bring carbon below 0.020 % while holding nitrogen in the 0.10–0.16 % band.
  2. Cast and forge. Ingot to the 6,300 t, 4,000 t or 2,000 t press, or ring-rolled from a punched preform, worked between 1,150 °C and 850 °C.
  3. Solution anneal and quench. 1,070–1,150 °C followed by rapid water quenching, with the furnace chart retained.
  4. Machine. As-forged with allowance, proof-machined for volumetric inspection, or finish-machined to drawing.
  5. Test and certify. Chemistry, mechanical testing, ultrasonic and magnetic particle examination, dimensional report, then certification.

§11 Testing, approvals and certification

Run in our own laboratory

  • Optical emission spectrometry to ASTM E415
  • Infrared carbon and sulfur analysis to ASTM E1019
  • Positive material identification by handheld analyser
  • Tensile testing to ASTM A370 and ISO 6892 on 600 kN and 300 kN machines
  • Charpy V-notch impact testing to −60 °C
  • Ultrasonic examination to ASTM A388 and EN 10228-3
  • Magnetic particle examination to ASTM E709
  • Metallography and grain size to ASTM E112

Placed with an accredited third-party laboratory

For 1.4466 these are the tests a urea or nitric acid project usually needs, and they are scheduled before shipment with the report issued alongside the mill certificate:

  • Intergranular corrosion to ASTM A262, including Practice C (Huey)
  • Corrosion testing to ASTM G28 Method A
  • Pitting resistance to ASTM G48 where specified
  • Impact testing below −60 °C
  • Bench Brinell or Rockwell hardness where a portable instrument is not accepted

State these on the enquiry. Corrosion testing has a lead time of its own and is the most common cause of a late shipment when it is added after the order.

Approvals and documents

  • Classification society approvals: CCS, BV, DNV, LR and NK
  • EN 10204 3.1 mill test certificate as standard
  • EN 10204 3.2 witnessed by BV, DNV, LR, SGS, TÜV or your own inspector on request
  • Traceability from melt number through forging, heat treatment and machining to shipment
  • Heat-treatment charts, NDT reports, dimensional reports and PMI records

§12 Ordering 1.4466 forgings

Quotations are prepared from a drawing or a written specification. Sending the seven items below in the first email removes a round trip and usually gets a price back within two working days. Minimum order is 10 kg with no minimum piece count, and lead time runs 20 to 60 days.

What to include in a 1.4466 request for quotation
#ItemExample
1Specification and gradeASTM A182 F310MoLN, UNS S31050, or EN 10088-3 X1CrNiMoN25-22-2 (1.4466)
2Drawing or dimensionsOD 1,450 × ID 1,120 × H 180 mm, or PDF / DWG / DXF / STEP
3Quantity and repeat volume6 pcs, roughly twice a year
4Delivery conditionSolution annealed + water quenched, proof-machined for UT
5Corrosion and NDT requirementsASTM A262 Practice C, licensor Huey limit, UT to ASTM A388
6Special requirementsδ-ferrite ≤ 0.5 FN; impact at −196 °C; licensor specification reference
7Certification and destinationEN 10204 3.2 witnessed by DNV, delivered Rotterdam

If you are cross-referencing a licensor specification against EN or ASTM limits, send it with the enquiry. We confirm the applicable specification in writing before production starts, not after the certificate is issued.

Email a 1.4466 enquiry Call +86 189 2135 9659

§13 Frequently asked questions

What is 1.4466 stainless steel?

1.4466, steel name X1CrNiMoN25-22-2, is a fully austenitic stainless steel containing 24–26 % chromium, 21–23 % nickel, 2.0–2.5 % molybdenum and 0.10–0.16 % nitrogen, with carbon limited to 0.020 %. It is known internationally as UNS S31050 and, for forgings, as ASTM A182 Grade F310MoLN. It was developed to resist ammonium carbamate corrosion in the high-pressure section of urea plants and is also used in nitric acid and NPK fertilizer service.

Is 1.4466 a duplex stainless steel?

No. 1.4466 is fully austenitic, with nickel at about 22 % and nitrogen added to keep the structure austenitic despite 25 % chromium. Producers report very low to zero ferrite content, and urea licensors often set a δ-ferrite ceiling on the finished part. That description, together with figures of 25–28 % Cr, 4.5–6.5 % Ni and 880 MPa tensile strength, belongs to a different steel: 1.4460, X3CrNiMoN27-5-2, whose EN 10088-3 tensile band is 620–880 MPa.

What is the ASTM equivalent of 1.4466?

For forgings, flanges, fittings and valve parts it is ASTM A182 / ASME SA-182 Grade F310MoLN, UNS S31050. For seamless tube and pipe it is ASTM A213 and A312 under the same UNS number. Composition limits differ slightly between EN and ASTM, most noticeably silicon and molybdenum, so a purchase order should name the governing specification as well as the grade.

What is the chemical composition of 1.4466?

To EN 10088-3, in mass percent: carbon 0.020 max, silicon 0.70 max, manganese 2.00 max, phosphorus 0.025 max, sulfur 0.010 max, chromium 24.0 to 26.0, nickel 21.0 to 23.0, molybdenum 2.00 to 2.50, nitrogen 0.10 to 0.16, iron balance.

What are the mechanical properties of 1.4466 forgings?

In the solution annealed condition to EN 10088-3, bars and forgings up to 160 mm show tensile strength 540–740 MPa, proof strength at least 250 MPa, elongation at least 35 % longitudinal, impact energy at least 100 J longitudinal and hardness up to 240 HBW. To ASTM A182 Grade F310MoLN the minima are 540 MPa tensile, 255 MPa yield, 25 % elongation and 40 % reduction of area; A182 sets no hardness limit for this grade.

What is the solution annealing temperature for 1.4466?

1,070 to 1,150 °C, held until the section is through-heated, followed by rapid quenching in water. Producer practice for thin sections is 1,070–1,120 °C for five to fifteen minutes. A fast quench matters because a 25 Cr–2 Mo austenite will precipitate sigma and chi phases if it dwells around 600–900 °C, and those phases cost both toughness and carbamate resistance. If the order is placed to ASTM A182, that standard sets its own narrower range of about 1,050–1,100 °C with a liquid quench, and the forging is treated to the standard's table instead.

In what temperature range is 1.4466 forged?

Between about 1,150 °C and 850 °C. Below 850 °C the alloy work-hardens rapidly and the risk of surface cracking rises, so heavy sections are reheated rather than forced. Forging is always followed by solution annealing and quenching.

Why is 1.4466 used in urea plants?

Ammonium carbamate at around 180–210 °C and 130–150 bar attacks ordinary stainless steel quickly, and attacks grain boundaries first. The combination of 25 % chromium, carbon below 0.020 % and nitrogen-stabilised fully austenitic structure resists both the general attack and the intergranular attack. The longest recorded service life in a urea stripper is 35 years, and the grade is written into the high-pressure material lists of Stamicarbon, Saipem, Kellogg and Urea Casale.

What is the PREN of 1.4466?

About 34. Using PREN = %Cr + 3.3 × %Mo + 16 × %N on the nominal analysis of 25 Cr, 2.1 Mo and 0.12 N gives 33.85. BÖHLER states PREN greater than 33 and Outokumpu lists 34 for its equivalent grade.

Which welding consumables suit 1.4466?

ISO 14343 S 25 22 2 N L wire for TIG and MIG welding, and ISO 3581 E 25 22 2 N L B covered electrodes for manual metal arc welding. The same wire or strip is used for corrosion-resistant overlay on tube sheets and pressure vessels. Weld without preheat, keep heat input below 1.0 kJ/mm and interpass temperature below 100 °C, and use string beads. Post-weld heat treatment is normally unnecessary.

Which corrosion tests are normally required on 1.4466 forgings?

Intergranular corrosion testing to ASTM A262, most often Practice C, the Huey test in boiling 65 % nitric acid, is the usual requirement, sometimes with ASTM G28 Method A alongside it. Urea licensors set their own maximum corrosion rate and maximum selective attack depth. We place these tests with an accredited third-party laboratory and issue the report with the mill certificate; they need to be stated at enquiry stage so they are scheduled rather than added late.

What is the largest 1.4466 forging you can supply?

Seamless rolled rings up to 6,000 mm outside diameter on the 6 m radial-axial mill, and single pieces up to 30 tonnes, worked on 6,300 t, 4,000 t and 2,000 t presses with a maximum melt size of 60 tonnes. Discs and tube sheets machine to Ø5,000 mm, shafts turn to 14,000 mm, and bores run to Ø1,600 × 10,000 mm.

What is the minimum order quantity and lead time for 1.4466?

Minimum order is 10 kg with no minimum piece count, so a single part is quotable. Lead time is 20 to 60 days from order confirmation. Standard melted-and-forged stainless grades sit at the lower end; third-party corrosion testing and witnessed inspection move the date, so both should be flagged at enquiry stage.

What certification comes with a 1.4466 forging?

An EN 10204 3.1 mill test certificate as standard, or EN 10204 3.2 witnessed by BV, DNV, LR, SGS, TÜV or your own inspector on request. Because the steel is melted on site, the certificate traces back to the melt number rather than stopping at a purchased billet. Heat-treatment charts, NDT reports, dimensional reports and PMI records are supplied with it.

What is the difference between 1.4466 and 1.4465?

1.4465 is X1CrNiMoN25-25-2, a 25 Cr–25 Ni–2 Mo grade listed in SEW 400 with higher nickel than 1.4466. Both are urea-grade austenitic steels and producers sometimes certify a single product to either on request, but they are separate grades with separate composition limits. Do not substitute one for the other without the purchaser's and the licensor's written approval.

§15 Sources

Standard and producer data on this page is reproduced from the references below and was last checked on . Values are given for information; the governing document is the specification named in your purchase order.

  1. SteelNumber, X1CrNiMoN25-22-2 (1.4466) composition, properties and standards. EN 10088-2:2005 data.
  2. H2ABC materials database, X1CrNiMoN25-22-2 1.4466 to DIN EN 10088-3:2014. Composition and mechanical property tables by size.
  3. voestalpine BÖHLER, BÖHLER A405 (1.4466 / S31050 / A182-F310MoLN) datasheet.
  4. Alleima, Alleima 2RE69 material datasheet. Composition, mechanical, physical, corrosion and welding data for S31050 / 1.4466.
  5. ASTM A182/A182M, mechanical requirements for Grade F310MoLN (UNS S31050): 78 ksi [540 MPa] tensile, 37 ksi [255 MPa] yield, 25 % elongation, 40 % reduction of area.
  6. HSM Stahl, 1.4466 datasheet. Thermal treatment ranges and room-temperature physical constants.
  7. Outokumpu, Ultra 725LN (1.4466 / S31050). Typical analysis and PRE value.

§16 Talk to the works

Jiangyin Jiangnan Metal Co., Ltd. is an integrated steel melting and open-die forging works in Zhouzhuang Town, Jiangyin City, Jiangsu Province, China, operating since 1997. Melting, forging, ring rolling, heat treatment, machining and testing all happen on one site. 460 people work here, including 9 senior engineers, 32 intermediate engineers and 140 technicians.

Plant and registered address

No.1 Chengxiqiao Road
Zhouzhuang Town, Jiangyin City
Jiangsu Province, China

Telephone, WhatsApp and WeChat

+86 189 2135 9659

Email

sales@steelforgepieces.com

Business hours

Monday to Saturday
08:00–17:30 China Standard Time (UTC+8)

Getting here

Wuxi Shuofang International Airport 30 km
Shanghai airports 160 km
Export ports: Zhangjiagang and Shanghai

Visits and audits

Customer audits, pre-shipment inspection and third-party witness testing are welcome. Arrange by email so an English-speaking engineer is available.

Send a 1.4466 enquiry