# XM-29 Forgings, UNS S24000 / Nitronic 33

Open die forged rings, seamless rolled rings, flanges, round bars, shafts, discs,
sleeves, bushings and tube sheets in nitrogen strengthened austenitic stainless steel.

Supplier: Jiangyin Jiangnan Metal Co., Ltd., open die forging factory
Address: No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
Tel: 0086-189-2135-9659
Email: sales@steelforgepieces.com
Page: https://www.steelforgepieces.com/Stainless-Steel/XM-29.html
Reviewed: 11 October 2026

## XM-29 at a glance

XM-29 is the ASTM designation for UNS S24000, a nitrogen strengthened austenitic
stainless steel with 17.00 to 19.00 % Cr, 11.50 to 14.50 % Mn, 2.25 to 3.75 % Ni and
0.20 to 0.40 % N. The same grade is sold under the trade name Nitronic 33 and by
Carpenter Technology as 18Cr-3Ni-12Mn. Manganese and nitrogen take the place of most of
the nickel used in Type 304, giving an annealed yield strength about twice that of 304
together with good toughness, good ductility and very low magnetic permeability that is
held after severe cold work and at cryogenic temperature.

Bar to ASTM A276 Type XM-29 must meet 100 ksi (690 MPa) tensile, 55 ksi (380 MPa) yield,
30 % elongation and 50 % reduction of area as minimum values. The grade hardens by cold
work only and does not respond to thermal hardening.

| Key fact | Value |
|---|---|
| UNS number | S24000 |
| ASTM designation | XM-29 |
| Trade names | Nitronic 33, Carpenter 18Cr-3Ni-12Mn |
| Family | Austenitic, nitrogen strengthened |
| Yield strength, A276 bar, min | 380 MPa / 55 ksi |
| Tensile strength, A276 bar, min | 690 MPa / 100 ksi |
| Density | 7.775 g/cm3 |
| Forging stock specification | ASTM A314 |

## 1. What XM-29 is

XM-29 belongs to the Cr-Mn-N austenitic family. Instead of 8 to 10 % nickel, austenite is
held stable by roughly 12 % manganese together with 0.20 to 0.40 % nitrogen in solid
solution. Nitrogen is an effective strengthener, so the grade reaches its high yield
strength in the annealed condition rather than through cold work or precipitation
hardening. The manganese level raises hot ductility and lets the steel dissolve more
nitrogen than a conventional 18-8 composition can hold.

Because the austenite is stable, the structure does not transform to martensite under
heavy deformation or at low temperature. That is why the grade keeps very low magnetic
permeability after severe cold working and down to cryogenic temperature.

### Designation cross reference

| Designation type | Value |
|---|---|
| UNS | S24000 |
| ASTM type symbol | XM-29, tubular products TP XM-29 |
| Trade name | Nitronic 33 |
| Producer designation | Carpenter 18Cr-3Ni-12Mn |
| SAE | XM-290 |
| ASTM product specifications | A240, A249, A269, A276, A312, A358, A412, A479, A580, A688, A813, A814 |
| Forging stock | ASTM A314, stainless steel billets and bars for forging |

## 2. Chemical composition of XM-29 (UNS S24000)

Weight percent. Ranges are those allowed by the applicable ASTM specifications.

| Element | Content (%) | Function |
|---|---|---|
| Carbon, C | 0.08 max | Held low to limit carbide precipitation |
| Silicon, Si | 0.75 max, 1.00 max in ASTM A276 | Deoxidiser |
| Manganese, Mn | 11.50 to 14.50 | Austenite stabiliser, raises nitrogen solubility and hot ductility |
| Phosphorus, P | 0.060 max | Residual |
| Sulfur, S | 0.030 max | Residual |
| Chromium, Cr | 17.00 to 19.00 | Passive film, corrosion resistance |
| Nickel, Ni | 2.25 to 3.75, listed as 2.3 to 3.7 in ASTM A276 and A240 | Austenite stability, toughness |
| Nitrogen, N | 0.20 to 0.40 | Main solid solution strengthener |
| Iron, Fe | Balance | Base |

Forging stock is procured from EAF plus VOD or ESR melted heats. The melting route is
stated on the mill certificate issued with every order.

## 3. Mechanical properties

### 3.1 Specified minimum values, solution annealed

| Property | ASTM A276 Type XM-29 bar | ASTM A240 UNS S24000 plate |
|---|---|---|
| Tensile strength, min | 100 ksi (690 MPa) | 690 MPa |
| Yield strength, min | 55 ksi (380 MPa) | 415 MPa |
| Elongation in 2 in. or 4D, min | 30 % | 40 % |
| Reduction of area, min | 50 % | not specified |

### 3.2 Typical annealed values

Results vary with section size, amount of hot work and test direction. These figures are
indicative and do not replace the order specification.

| Property | Metric | Imperial |
|---|---|---|
| Tensile strength | 689 MPa typical, up to about 770 MPa reported | 100 ksi, up to about 110 ksi |
| Yield strength, 0.2 % proof | 379 MPa typical, up to about 430 MPa reported | 55 ksi, up to about 63 ksi |
| Elongation at break in 2 in. | 39 to 40 % | 39 to 40 % |
| Reduction of area | about 57 % | about 57 % |
| Hardness, Brinell | 210 to 241 HB | 210 to 241 HB |
| Hardness, Rockwell B | 88 to 100 HRB | 88 to 100 HRB |
| Modulus of elasticity | 200 GPa | 29 x 10^6 psi |
| Shear modulus | 77 GPa | 11 x 10^6 psi |
| Shear strength | 530 MPa | 77 ksi |
| Fatigue strength | 370 MPa | 54 ksi |
| Poisson ratio | 0.28 | 0.28 |

## 4. Physical and thermal properties

| Property | Metric | Imperial |
|---|---|---|
| Density | 7.775 g/cm3 | 0.2808 lb/in3 |
| Thermal expansion, 26 to 93 C (78 to 200 F) | 16.074 um/m.C | 8.93 uin/in.F |
| Specific heat capacity | 480 J/kg.K | 0.12 BTU/lb.F |
| Melting onset, solidus | 1350 C | 2460 F |
| Melting completion, liquidus | 1390 C | 2540 F |
| Latent heat of fusion | 280 J/g | - |
| Magnetic permeability | Very low, held after severe cold work and at cryogenic temperature | |

## 5. XM-29 compared with Type 304

XM-29 is superior to Type 304 in five specific points.

1. Yield strength in the annealed condition is about twice that of 304.
2. Strength and ductility at cryogenic temperature are excellent, with no deformation
   induced martensite.
3. Resistance to stress corrosion cracking is better than 304. The margin over 304 and
   304L in hot chloride solutions is clear at lower stress levels; at about 50 ksi and
   above the two grades are equal.
4. Low magnetic permeability is held at cryogenic temperature and after severe cold work.
5. Resistance to wear and galling is better than the standard austenitic stainless steels.

Nickel content of about 3 % instead of 8 to 10 % also keeps the grade less exposed to
nickel price movement, and base metal cost is moderately low among wrought austenitic
stainless steels.

## 6. Corrosion resistance and service limits

General corrosion resistance of XM-29 is superior to Type 409 and close to Type 304. In
weak acid solutions it approaches 304. In more aggressive media it is somewhat less
resistant than 304.

Service limit: like most stainless steels, XM-29 is prone to pitting and crevice
corrosion in seawater and other aggressive chloride media and should not be used in those
conditions unless cathodically protected. For seawater, firewater, subsea pipework,
risers and manifolds, specify a duplex or super duplex grade such as A182 F51, F53 or
F55, or the 6Mo austenitic grade A182 F44. For hot sulphuric and mixed acid duty,
consider Alloy 20, 904L or Hastelloy C-276.

## 7. Forging, heat treatment and fabrication

Forging: heat to 1093 C (2000 F) and soak until the section has equalized, then heat
again to 1177 C (2150 F), equalize and forge.

Solution annealing: soak at 1038 to 1121 C (1900 to 2050 F), then quench rapidly in water
or air.

| Operation | Practice |
|---|---|
| Forming | Commonly used forming methods apply. Process annealing at about 1065 C (1950 F) removes the stress that builds up because of the high work hardening rate. |
| Machining | Slow speeds, positive feeds and a resulphurised lubricant. Chips can be stringy and tough, so chip breakers or curlers are useful. |
| Welding | Submerged arc welding, gas metal arc welding and gas tungsten arc welding. The same equipment and techniques as conventional austenitic grades generally apply. |
| Hardening | By cold work only. Cannot be hardened by thermal treatment. |

## 8. XM-29 forged product forms

All items are produced by open die forging or ring rolling to the customer drawing,
supplied solution annealed unless another condition is agreed.

| Product form | Typical use |
|---|---|
| Forged rings and seamless rolled rings | Containment rings, retaining rings, non-magnetic structural rings |
| Forged flanges and flange blanks | Piping and pressure containing connections |
| Forged round bars, square bars and billets | Machining stock, fasteners, pins, valve stems |
| Forged shafts, spindles and eccentric shafts | Rotating equipment requiring low magnetic permeability |
| Forged discs, disks and tube sheets | Heat exchanger and vessel internals |
| Forged sleeves, bushings and hollow bars | Wear and galling resistant bushings |
| Forged tubes, pipes and nozzles | Tube assemblies and pipework components |
| Forged valve bodies, seat rings, blocks and valve parts | Ball, gate, globe, check and plug valves, strainers |
| Forged gears, rolls, wheels and manifolds | Mechanical and structural components |

## 9. Typical applications

Published applications for this grade include tube assemblies, pipes, cable, valves,
tanks, containment rings and fans. In practice the grade is specified when a project
needs a non-magnetic austenitic structure that survives heavy cold work, about double the
annealed yield strength of 304 at a lower nickel content, dependable toughness at
cryogenic temperature, or better galling and wear behaviour than standard austenitic
grades. Typical forged parts go into cryogenic and liquefied gas equipment, generator and
electrical hardware, bulk solid handling and screening equipment, hoppers, chutes and
trailer bed liners, wastewater and sewage treatment structures, and general mechanical
and structural parts. For chloride rich or seawater duty see section 6.

## 10. Testing, inspection and certification

- Chemical analysis and room temperature tensile test on every heat, with hardness and,
  on request, Charpy impact and cryogenic testing.
- Ultrasonic examination to EN 10228-3, SEP 1921 or ASTM A388 as nominated on the order.
- Dimensional inspection against the customer drawing, with PMI and liquid penetrant
  testing on request.
- Material certification to EN 10204 3.1, or EN 10204 3.2 endorsed by a third party such
  as TUV, BV, DNV or Lloyd's Register.
- Forging stock ordered to ASTM A314.

## 11. Frequently asked questions

**What is XM-29 stainless steel?**
XM-29 is the ASTM designation for UNS S24000, a nitrogen strengthened austenitic
stainless steel with 17.00 to 19.00 % chromium, 11.50 to 14.50 % manganese, 2.25 to
3.75 % nickel and 0.20 to 0.40 % nitrogen. Annealed yield strength is about twice that of
Type 304.

**Is XM-29 the same as Nitronic 33?**
Yes. XM-29, UNS S24000 and Nitronic 33 describe the same 18Cr-3Ni-12Mn grade. Carpenter
Technology markets the same composition as 18Cr-3Ni-12Mn.

**What are the minimum mechanical properties of XM-29 bar?**
ASTM A276 Type XM-29 bar: 100 ksi (690 MPa) tensile, 55 ksi (380 MPa) yield, 30 %
elongation in 2 in., 50 % reduction of area, all minimum. ASTM A240 plate in UNS S24000:
690 MPa tensile, 415 MPa yield, 40 % elongation minimum.

**At what temperature is XM-29 forged?**
Heat to 1093 C (2000 F) and soak to equalize, then heat again to 1177 C (2150 F),
equalize and forge. Solution anneal at 1038 to 1121 C (1900 to 2050 F) and quench rapidly
in water or air.

**Can XM-29 be hardened by heat treatment?**
No. It hardens by cold work only.

**Is XM-29 magnetic?**
Magnetic permeability stays very low even after severe cold working and at cryogenic
temperature.

**Is XM-29 suitable for seawater or subsea service?**
In general no. It is prone to pitting and crevice corrosion in seawater and other
aggressive chloride media and should not be used there unless cathodically protected.
Duplex grades A182 F51, F53 and F55, or the 6Mo austenitic A182 F44, are the usual
alternatives.

**Which ASTM specifications cover XM-29?**
A240, A249, A269, A276, A312, A358, A412, A479, A580, A688, A813 and A814. Billets and
bars for forging are ordered to ASTM A314.

**What information is needed for a quotation?**
A drawing or rough dimensions, OD x ID x height for rings and diameter x length for bars
and shafts, plus quantity, governing specification and delivery condition, NDT and
certification requirements, and destination port.

## Request a quotation

Jiangyin Jiangnan Metal Co., Ltd., open die forging factory, Jiangyin, Jiangsu, China.
XM-29 (UNS S24000 / Nitronic 33) rings, flanges, bars, shafts, discs and sleeves to
drawing.

- Address: No.1 Chengxiqiao Road, Zhouzhuang Town, Jiangyin City, Jiangsu Province, China
- Tel: 0086-189-2135-9659
- Email: sales@steelforgepieces.com
- Contact page: https://www.steelforgepieces.com/Contact-Us/

## Data sources

Composition, mechanical, thermal and fabrication data are taken from the ASTM A276 and
ASTM A240 requirements for XM-29 and UNS S24000, from ASTM A314, and from published
Nitronic 33 and UNS S24000 datasheets. Figures are indicative and do not replace the full