# UNS S41600 (AISI 416) Forgings

Grade sheet. Supplier: Jiangyin Jiangnan Metal Co., Ltd., No.1 Chengxiqiao Road,
Zhouzhuang Town, Jiangyin City, Jiangsu Province 214423, China.
Phone +86 189 2135 9659. Email sales@steelforgepieces.com.
Source page: https://www.steelforgepieces.com/Stainless-Steel/UNS-S41600.html
Revision date: 9 October 2026.

## Summary

UNS S41600 is the UNS designation for AISI type 416, a free-machining martensitic
stainless steel with 12.0 to 14.0 % chromium, 0.15 % maximum carbon and a minimum
0.15 % sulfur addition. The sulfur forms manganese sulfide inclusions that break up
the chip and give a machinability of about 85 % of free-machining carbon steel, the
highest of any stainless steel. Formability, weldability and corrosion resistance are
lower than grade 410. The steel is hardenable by quenching and tempering and is
magnetic in all conditions.

Jiangyin Jiangnan Metal forges UNS S41600 to ASTM A473 from steel melted in its own
electric arc furnace, in single pieces from 10 kg to 30 tonnes, with rolled rings to
6,000 mm outside diameter, under EN 10204 3.1 or witnessed 3.2 certification.

| Item | Value |
| --- | --- |
| Grade | UNS S41600 / AISI 416 |
| Type | Martensitic, free-machining, hardenable, magnetic |
| Forging specification | ASTM A473 |
| Bar specifications | ASTM A582, A484, A314; AMS 5610 Type II; QQ-S-764B (former) |
| Equivalents | EN 1.4005, X12CrS13, BS 416S21 / En 56AM, JIS SUS 416, SS 2380 |
| Machinability | about 85 % of free-machining carbon steel |
| Main limitation | poor weldability, not for chloride or marine service |
| MOQ | 10 kg, no minimum piece count |
| Lead time | 20 to 60 days |

## Chemical composition (ASTM A473, type 416)

| Element | Min % | Max % |
| --- | --- | --- |
| Carbon | - | 0.15 |
| Chromium | 12.0 | 14.0 |
| Manganese | - | 1.25 |
| Silicon | - | 1.00 |
| Phosphorus | - | 0.06 |
| Sulfur | 0.15 | - |
| Molybdenum | - | 0.60 (at manufacturer option, reported only when intentionally added) |
| Iron | Balance | |

Chemistry on every heat is checked in house by optical emission spectrometry to
ASTM E415 and by infrared carbon and sulfur analysis to ASTM E1019, reported on the
mill certificate against the melt number.

## Mechanical requirements for forgings, ASTM A473 Condition A

| Property | Requirement |
| --- | --- |
| Yield strength, 0.2 % offset, min | 40 ksi (275 MPa) |
| Tensile strength, min | 70 ksi (485 MPa) |
| Elongation in 2 in. (50 mm) or 4D, min | 20 % |
| Reduction of area, min | 45 % |
| Brinell hardness, max | 223 HBW |
| Response to heat treatment, min | 35 HRC after hardening from 1750 F (955 C) |

Martensitic grades under A473 are supplied annealed, or hardened and tempered as
specified. Liquid quenching requires agreement with the purchaser. Test specimens come
from prolongations on the forging: for solid forgings the specimen axis sits midway
between centre and surface, parallel to the direction of greatest metal flow; for upset
discs and rings it is taken from the periphery.

## Reference properties of grade 416 bar after tempering (ASTM A582 data)

These are bar values, not forging requirements. A forging is accepted against its own
prolongation test.

| Condition / tempering temperature | Tensile MPa | 0.2 % proof MPa | Elongation % in 50 mm | Hardness HB | Charpy V J |
| --- | --- | --- | --- | --- | --- |
| Annealed (Condition A, typical) | 517 | 275 | 30 | 262 | - |
| Condition T, hardened and tempered | 758 | 586 | 18 | 248-302 | - |
| Tempered 204 C | 1340 | 1050 | 11 | 388 | 20 |
| Tempered 316 C | 1350 | 1060 | 12 | 388 | 22 |
| Tempered 427 C (avoid) | 1405 | 1110 | 11 | 401 | low |
| Tempered 538 C (avoid) | 1000 | 795 | 13 | 321 | low |
| Tempered 593 C | 840 | 705 | 19 | 248 | 27 |
| Tempered 650 C | 796 | 670 | 17.5 | 253 | 38 |

Tempering between 400 C and 580 C must be avoided because impact resistance falls
sharply in that band.

## Physical properties, annealed

| Property | Value |
| --- | --- |
| Density | 7,800 kg/m3 (0.276 lb/in3) |
| Modulus of elasticity | 200 GPa |
| Thermal expansion | 9.9 um/m.C (0-100 C), 11.0 (0-315 C), 11.5 (0-538 C) |
| Thermal conductivity | 24.9 W/m.K at 100 C, 28.7 W/m.K at 500 C |
| Specific heat 0-100 C | 460 J/kg.K |
| Electrical resistivity | 570 nOhm.m |
| Melting point | about 1,490 C (2,714 F) |
| Magnetic response | ferromagnetic in all conditions |

## International equivalents

| System | Designation |
| --- | --- |
| UNS | S41600 |
| AISI / SAE | 416 |
| Euronorm number | 1.4005 |
| Euronorm name | X12CrS13 |
| Old British | 416S21, En 56AM |
| Swedish SS | 2380 |
| Japanese JIS | SUS 416 |

EN 1.4005 to EN 10088-3 allows a wider sulfur band than the ASTM grade. Where a drawing
calls both EN 1.4005 and ASTM A473 type 416, confirm which chemistry governs before the
heat is poured.

## Processing

Hot working: heat uniformly to 1,149 to 1,232 C (2,100 to 2,250 F), forge, air cool,
cool large sections slowly. Do not hot work below about 927 C (1,700 F).

Annealing: full anneal 815 to 900 C, about half an hour per 25 mm, cool no faster than
30 C per hour to 600 C, then air cool. Sub-critical anneal 650 to 760 C and air cool
before machining.

Hardening and tempering: austenitise 925 to 1,010 C, oil quench, temper to the required
strength. Avoid 400 to 580 C. Commercial hardened and tempered 416 is normally about
26 to 32 HRC.

Machining: best in the sub-critically annealed condition, about 85 % machinability,
the highest of any stainless steel.

Welding: poor and normally avoided. If unavoidable, preheat 200 to 300 C, use grade 410
low-hydrogen electrodes or grade 309 filler, then re-harden, anneal, or stress relieve
at 650 to 675 C.

Corrosion: resists fresh water, dry atmospheres, mild acids and alkalis. Below grade 410
and well below the austenitic grades. Not suitable for marine or chloride exposure. Best
resistance when hardened and polished. Scaling limit about 760 C intermittent, 675 C
continuous. Not a NACE MR0175 sour-service grade.

Forging note: the manganese sulfide inclusions are elongated by forging reduction, so
transverse ductility and transverse impact are lower than longitudinal. State the loading
direction at enquiry stage so the forging sequence and test specimen orientation can be
planned.

## Products supplied in UNS S41600

Forged round, square, rectangular, flat and hexagon bars. Hollow bars, sleeves, bushes,
bushings, cylinders, barrels, casings, shells, hubs and housings. Forged rings and
seamless rolled rings, OD 50 to 6,000 mm. Discs, blocks and plates. Valve stems, valve
seats, valve seat rings, valve bodies, valve bonnets. Pump shafts, motor shafts, gears,
bolts, nuts, studs and automatic screw-machine components.

## Plant capability

| Stage | Equipment | Limit |
| --- | --- | --- |
| Melting | 25 t EAF, 25 t and 50 t LF, 30 t and 60 t VOD, 2 / 8 / 25 t induction | 60 t max heat |
| Forging | 6,300 t, 4,000 t, 2,000 t presses; 5 t to 750 kg hammers | 30 t single piece |
| Ring rolling | radial-axial mills 6 m, 3 m, 1 m | OD 50 to 6,000 mm |
| Heat treatment | 14 furnaces, car-bottom to 8,000 x 2,000 x 2,000 mm, two 15 m well furnaces | recorded charts |
| Machining | VTL to 5,000 mm swing, lathes to 14 m, CNC deep-hole drilling | bore 1,600 x 10,000 mm |
| Testing | OES E415, C/S E1019, PMI, tensile 600 kN and 300 kN, Charpy to minus 60 C, UT A388, MT E709, metallography E112 | in-house laboratory |
| Certification | CCS, BV, DNV, LR, NK; EN 10204 3.1 standard, 3.2 witnessed on request | melt-number traceability |

Operating since 1997. 460 staff, including 9 senior engineers, 32 intermediate engineers
and 140 technicians. Exports to North America, Europe, the Middle East and Asia-Pacific.

## Enquiry checklist

1. Grade and specification, for example UNS S41600, ASTM A473, Condition A.
2. Dimensions or drawing in PDF, DWG, DXF or STEP.
3. Quantity and expected repeat volume.
4. Delivery condition, as forged or proof-machined with allowance.
5. Heat treatment and testing requirements.
6. Certification level and destination port.

Quotations are returned within two working days.
Email sales@steelforgepieces.com or call +86 189 2135 9659.

## Sources

ASTM A473 Standard Specification for Stainless Steel Forgings, Tables 1, 2 and 3.
ASTM A582 free-machining stainless bar, published reference data for grade 416.
ASTM A484, ASTM A314, AMS 5610 Type II.

Data is guidance for grade selection and does not replace the governing specification.